| Category | Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE | 
| Manufacturer | ScanTube | 
| Trade Name | |
| Port | Ningbo port,China | 
| Trade Terms | FOB, CFR, CIF | 
| Payment Terms | L/C, T/T, Western Union | 
| Download PDF | ScanTube ETFE Tubing.pdf  | 
| Price | EMAIL US sales@lookpolymers.com | 
| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 | 
| Water Absorption | <= 0.030 % | <= 0.030 % | ASTM D257 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Hardness, Shore D | 75 | 75 | ASTM D2240 | 
| Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638, ASTM D1708 | 
| Elongation at Break | 200 % | 200 % | ASTM D638, ASTM D1708 | 
| Tensile Modulus | 0.827 GPa | 120 ksi | ASTM D638 | 
| Flexural Modulus | 1.38 GPa | 200 ksi | ASTM D790 | 
| Compressive Strength | 48.3 MPa | 7000 psi | ASTM D695 | 
| Izod Impact, Notched | NB | NB | ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 | 
| Melting Point | 260 °C | 500 °F | |
| Maximum Service Temperature, Air | 150 °C | 302 °F | Continuous | 
| Deflection Temperature at 0.46 MPa (66 psi) | 104 °C | 219 °F | ASTM D648 | 
| Deflection Temperature at 1.8 MPa (264 psi) | 71.0 °C | 160 °F | ASTM D648 | 
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | >= 30 % | >= 30 % | ASTM D2863 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | ASTM D257 | 
| Dielectric Constant | 2.6 @Frequency 1000 Hz | 2.6 @Frequency 1000 Hz | ASTM D150 | 
| 2.6 @Frequency 1.00e+6 Hz | 2.6 @Frequency 1.00e+6 Hz | ASTM D150 | |
| Dielectric Strength | 78.7 kV/mm | 2000 kV/in | Short Term; 10 mil film; ASTM D149 | 
| Dissipation Factor | 0.00080 @Frequency 1000 Hz | 0.00080 @Frequency 1000 Hz | ASTM D150 | 
| 0.0050 @Frequency 1.00e+6 Hz | 0.0050 @Frequency 1.00e+6 Hz | ASTM D150 | 
| Descriptive Properties | Value | Comments | 
|---|---|---|
| Chemical Resistance | Excellent | |
| Weather Resistance | Excellent |