Polymer Property : Hardness, H358/30 = 100 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Cycolac® MG8000SR ABS
This data was supplied by SABIC-IP for the Americas region.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East)
This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East)
CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® ML1010 PC (Europe-Africa-Middle East)
Superior performance, improved flow over standard grades at lower temperatures. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® OQ1023 PC (Asia Pacific)
Lexan OQ1023 resin is an optical high purity PC resin optimized for demanding recordable and rewritable formats (CD-R, DVD-R, DVD-RW). It is also suitable for short cycletime CD and DVD production
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Lexan® OQ1026 PC (Asia Pacific)
LEXAN OQ1026 is an optical quality, high purity PC resin optimized for the demanding short cycle times used in DVD production. Advances in technology further enhanced the processability while mainta..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East)
Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm ..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East)
NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East)
NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East)
VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East)
VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN2 is a standard 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2 can be used for all applications where a higher modulus is required. NORYL GFN2 is ava..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL GFN2V PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN2V is a 20 % glass fibre reinforced material with a HDT/A of 130C according ISO 75. NORYL GFN2V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East)
NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL HF185 PPE+HIPS (Europe-Africa-Middle East)
NORYL HF185 is an unfilled, halogen free (according VDE/DIN 472 part 815), flame retardant and easy flow NORYL grade.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East)
PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)...
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Xenoy® XL1562 PBT+PC (Europe-Africa-Middle East)
XENOY XL1562 is an impact modified PBT+PC blend with outstanding chemical resistance, good UV stability and flow properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Europe-Africa-Middle East)
NORYL 731 is an unfilled material, with a Vicat B/120 of 140C according ISO 306. NORYL 731 is a general purpose material with good balance of Strength, Impact and Flow. NORYL 731 is available in all..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL GFN1 PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN1 is a standard 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1 can be used for all applications where a higher modulus is required. NORYL GFN1 is ava..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.