Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638-95 |
Multibase Multi-Pro® 2005 RC I High Impact 20% Glass Polypropylene Multi-Pro 2005 RC I is a chemically coupled polypropylene compound with increased stiffness, flex strength and excellent impact resistance. This product is geared for top engineering plastics appli.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Nylene® CX3451 Translucent Nylon Copolymer Description: Nylene® CX 3451 is a translucent specialty nylon. CX3451 is FDA/NSF approved. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Nylene® Naxel™ PC10 Polycarbonate Description: Naxel™ PC10 is a 9 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources C.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | |
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D412 |
2065D Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Ultimate | 58.6 - 72.4 MPa | 8500 - 10500 psi | Average value: 64.5 MPa Grade Count:8 |
Overview of materials for Polycarbonate, Aramid Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PE-40GF/000 NATURAL High Density Polyethylene (HDPE), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedNaturalPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 58.6 - 92.2 MPa | 8500 - 13400 psi | Average value: 80.9 MPa Grade Count:7 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Tensile Strength, Ultimate | 58.6 - 221 MPa | 8500 - 32100 psi | Average value: 116 MPa Grade Count:81 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Tensile Strength, Ultimate | 58.6 - 82.7 MPa | 8500 - 12000 psi | Average value: 66.4 MPa Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Electrafil® PC-50/EC Polycarbonate, Conductive Carbon Filled Conductive Carbon, Powder Modified |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM Data |
Styron CALIBRE™ 891 10 Polycarbonate, General Purpose CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM Data |
Styron CALIBRE™ 891 20 Polycarbonate, General Purpose CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4800-10 Polycarbonate EMERGEâ„¢ 4800-10 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-10 Polycarbonate CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | after optimum cure |
Armstrong C-7/H20 Epoxy Adhesive A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | |
Abatron AboCast 7703-21/AboCure 7703-22 (B) Epoxy Adhesive and Casting Compound AboCast 7703-21/AboCure 7703-21 is an all-purpose clear, low-viscosity, variable-ratio epoxy adhesive and casting compound for electric and structural applications. As an Adhesive: it bonds permane.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | ASTM D638 |
Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | TM R050-36 |
Resinlab® EP691 Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP691 is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting and ad.. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | TM R050-36 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Tensile Strength, Ultimate | 58.6 MPa | 8500 psi | TM R050-36 |
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett.. |
|||
Tensile Strength, Ultimate | 58.6 MPa @Temperature 150 °C |
8500 psi @Temperature 302 °F |
ISO 62 |
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo.. |
|||
Tensile Strength, Ultimate | 58.6 - 72.4 MPa | 8500 - 10500 psi | ASTM D638 |
Premix Premi-Glas® 1200-24 Polyester SMC
(discontinued **) Premi-Glas® 1200-24 is a 24% fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck - Bus body panels and Marine cowls parts where smooth, flat, ripple free surfa.. |