PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.272 g/cc
1.272 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.6 MPa
8500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 4.83 GPa
700 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 4.83 GPa
700 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.10 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 343 - 382 °C
650 - 720 °F
Molding
Mold Temperature 135 - 149 °C
275 - 300 °F
Drying Temperature 135 - 149 °C
275 - 300 °F
Dry Time 2 hour
2 hour
Descriptive Properties Value Comments
Product Form Pellets