Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Nylon 11 with 10% Glass Fiber Filler

Category Polymer , Thermoplastic , Nylon , Nylon 11 , Nylon 11 with 10% Glass Fiber Filler
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 11 with 10% Glass Fiber Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.10 - 1.42 g/cc
0.0397 - 0.0513 lb/in³
Average value: 1.26 g/cc Grade Count:4
Linear Mold Shrinkage 0.00400 - 0.00800 cm/cm
0.00400 - 0.00800 in/in
Average value: 0.00583 cm/cm Grade Count:4
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
Average value: 108 Grade Count:3
Tensile Strength, Ultimate 58.6 - 82.7 MPa
8500 - 12000 psi
Average value: 66.4 MPa Grade Count:4
Elongation at Break 2.00 - 17.3 %
2.00 - 17.3 %
Average value: 8.22 % Grade Count:6
Modulus of Elasticity 2.76 - 4.14 GPa
400 - 600 ksi
Average value: 3.22 GPa Grade Count:6
Flexural Yield Strength 82.7 - 100 MPa
12000 - 14500 psi
Average value: 92.2 MPa Grade Count:4
Flexural Modulus 2.41 - 3.45 GPa
350 - 500 ksi
Average value: 3.02 GPa Grade Count:4
Izod Impact, Notched 0.534 - 0.747 J/cm
1.00 - 1.40 ft-lb/in
Average value: 0.614 J/cm Grade Count:4
Izod Impact, Unnotched 3.74 - 5.87 J/cm
7.00 - 11.0 ft-lb/in
Average value: 4.81 J/cm Grade Count:4
Charpy Impact Unnotched 9.17 - 10.0 J/cm²

@Temperature -30.0 - -30.0 °C
43.6 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.59 J/cm² Grade Count:2
Charpy Impact, Notched 0.440 - 0.550 J/cm²

@Temperature -30.0 - -30.0 °C
2.09 - 2.62 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.495 J/cm² Grade Count:2
Thermal Properties Metric English Comments
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:4
Processing Properties Metric English Comments
Mold Temperature 37.8 - 65.6 °C
100 - 150 °F
Average value: 51.7 °C Grade Count:4
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:4
Users viewing this material also viewed the following: