Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 80.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 0.345 - 80.0 MPa
50.0 - 11600 psi
Average value: 7.65 MPa Grade Count:872
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Tensile Strength, Ultimate 25.0 - 80.0 MPa

@Temperature 60.0 - 150 °C
3630 - 11600 psi

@Temperature 140 - 302 °F
Average value: 55.0 MPa Grade Count:2
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Tensile Strength, Ultimate 0.345 - 80.0 MPa
50.0 - 11600 psi
Average value: 11.6 MPa Grade Count:42
Overview of materials for Styrenic TPE  (Unverified Data**)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe..
Tensile Strength, Ultimate 55.2 - 80.0 MPa
8000 - 11600 psi
Average value: 66.9 MPa Grade Count:79
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Ultimate 50.0 - 80.0 MPa

@Temperature 60.0 - 120 °C
7250 - 11600 psi

@Temperature 140 - 248 °F
Average value: 66.7 MPa Grade Count:1
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Tensile Strength, Ultimate 44.1 - 80.0 MPa
6400 - 11600 psi
Average value: 67.0 MPa Grade Count:14
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Tensile Strength, Ultimate 8.48 - 80.0 MPa
1230 - 11600 psi
Average value: 16.6 MPa Grade Count:51
Overview of materials for PVC, Uncompounded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Ultimate 9.00 - 80.0 MPa
1310 - 11600 psi
Average value: 30.1 MPa Grade Count:177
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 68.7 - 80.0 MPa
9970 - 11600 psi
Average value: 75.3 MPa Grade Count:3
Overview of materials for Phenolic, Graphite Cloth Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value..
Tensile Strength, Ultimate 70.0 - 80.0 MPa

@Temperature 130 - 175 °C
10200 - 11600 psi

@Temperature 266 - 347 °F
Average value: 66.6 MPa Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Tensile Strength, Ultimate 70.0 - 80.0 MPa

@Time 1.80e+7 - 7.20e+7 sec
10200 - 11600 psi

@Time 5000 - 20000 hour
Average value: 66.6 MPa Grade Count:2
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Tensile Strength, Ultimate 22.0 - 80.0 MPa

@Temperature 80.0 - 120 °C
3190 - 11600 psi

@Temperature 176 - 248 °F
Average value: 50.9 MPa Grade Count:1
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Ultimate 22.0 - 80.0 MPa

@Strain 1.00 - 8.00 %
3190 - 11600 psi

@Strain 1.00 - 8.00 %
Average value: 50.9 MPa Grade Count:1
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Ultimate 30.0 - 80.0 MPa
4350 - 11600 psi
Alliance BIF-11 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 30.0 - 80.0 MPa
4350 - 11600 psi
Alliance BIF-17 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 30.0 - 80.0 MPa
4350 - 11600 psi
Alliance BIF-19 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 30.0 - 80.0 MPa
4350 - 11600 psi
Alliance BIF-2 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 30.0 - 80.0 MPa
4350 - 11600 psi
Alliance BIF-16 Bonded (Composite) Magnetic Material
Tensile Strength, Ultimate 42.0 - 80.0 MPa
6090 - 11600 psi
Average value: 71.4 MPa Grade Count:12
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Tensile Strength, Ultimate 23.0 - 80.0 MPa

@Temperature 160 - 160 °C
3340 - 11600 psi

@Temperature 320 - 320 °F
Average value: 68.8 MPa Grade Count:2
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 23.0 - 80.0 MPa

@Strain 0.600 - 3.00 %
3340 - 11600 psi

@Strain 0.600 - 3.00 %
Average value: 68.8 MPa Grade Count:2
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 50.0 - 80.0 MPa

@Temperature 160 - 160 °C
7250 - 11600 psi

@Temperature 320 - 320 °F
Average value: 70.2 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Tensile Strength, Ultimate 50.0 - 80.0 MPa

@Strain 0.600 - 1.40 %
7250 - 11600 psi

@Strain 0.600 - 1.40 %
Average value: 70.2 MPa Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Tensile Strength, Ultimate 40.0 - 80.0 MPa

@Temperature 60.0 - 120 °C
5800 - 11600 psi

@Temperature 140 - 248 °F
Average value: 60.0 MPa Grade Count:2
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Tensile Strength, Ultimate 0.800 - 80.0 MPa
116 - 11600 psi
Average value: 29.0 MPa Grade Count:318
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Tensile Strength, Ultimate 29.0 - 80.0 MPa

@Temperature -40.0 - 120 °C
4210 - 11600 psi

@Temperature -40.0 - 248 °F
Average value: 45.0 MPa Grade Count:4
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 9.00 - 80.0 MPa

@Temperature 60.0 - 120 °C
1310 - 11600 psi

@Temperature 140 - 248 °F
Average value: 31.0 MPa Grade Count:2
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..
Copyright © lookpolymers.com All Rights Reserved