| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.870 - 11.0 g/cc | 0.0314 - 0.397 lb/in³ | Average value: 1.06 g/cc Grade Count:952 |
| Water Absorption | 0.0500 % | 0.0500 % | Average value: 0.0500 % Grade Count:10 |
| Viscosity | 0.0300 - 30000 cP | 0.0300 - 30000 cP | Average value: 5130 cP Grade Count:23 |
| 1600 - 2300 cP @Temperature 180 - 180 °C |
1600 - 2300 cP @Temperature 356 - 356 °F |
Average value: 2080 cP Grade Count:4 | |
| Viscosity Measure | 6.00 - 80.0 cSt | 6.00 - 80.0 cSt | Average value: 21.0 cSt Grade Count:31 |
| Linear Mold Shrinkage | 0.00300 - 0.0470 cm/cm | 0.00300 - 0.0470 in/in | Average value: 0.0189 cm/cm Grade Count:112 |
| Linear Mold Shrinkage, Transverse | 0.00100 - 0.0190 cm/cm | 0.00100 - 0.0190 in/in | Average value: 0.00861 cm/cm Grade Count:23 |
| Melt Flow | 0.100 - 84.0 g/10 min | 0.100 - 84.0 g/10 min | Average value: 15.8 g/10 min Grade Count:70 |
| Spiral Flow | 49.0 - 107 cm @Temperature 200 - 200 °C |
19.3 - 42.1 in @Temperature 392 - 392 °F |
Average value: 73.6 cm Grade Count:8 |
| 49.0 - 107 cm @Pressure 7.00 - 7.00 MPa |
19.3 - 42.1 in @Pressure 1020 - 1020 psi |
Average value: 73.6 cm Grade Count:8 | |
| Ash | 0.350 - 39.0 % | 0.350 - 39.0 % | Average value: 15.0 % Grade Count:12 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 6.00 - 98.0 | 6.00 - 98.0 | Average value: 59.1 Grade Count:950 |
| Hardness, Shore D | 10.0 - 69.0 | 10.0 - 69.0 | Average value: 39.7 Grade Count:44 |
| Tensile Strength, Ultimate | 0.345 - 80.0 MPa | 50.0 - 11600 psi | Average value: 7.65 MPa Grade Count:872 |
| Tensile Strength, Yield | 0.207 - 29.0 MPa | 30.0 - 4210 psi | Average value: 3.62 MPa Grade Count:320 |
| Elongation at Break | 3.80 - 1900 % | 3.80 - 1900 % | Average value: 610 % Grade Count:948 |
| Modulus of Elasticity | 0.0180 - 0.207 GPa | 2.61 - 30.0 ksi | Average value: 0.0508 GPa Grade Count:9 |
| Rebound | 22.0 - 65.0 % | 22.0 - 65.0 % | Average value: 46.9 % Grade Count:27 |
| Flex Crack Resistance | 35000 - 132000 | 35000 - 132000 | Average value: 79400 Grade Count:4 |
| Adhesive Bond Strength | 0.550 - 2.65 MPa | 79.8 - 384 psi | Average value: 1.13 MPa Grade Count:10 |
| Izod Impact, Notched | 0.641 - 5340 J/cm | 1.20 - 10000 ft-lb/in | Average value: 1.01 J/cm Grade Count:11 |
| Izod Impact, Unnotched | 1.60 - 5340 J/cm | 3.00 - 10000 ft-lb/in | Average value: 2.14 J/cm Grade Count:10 |
| Penetration | 50.0 | 50.0 | Average value: 50.0 Grade Count:4 |
| Tear Strength | 2.00 - 113 kN/m | 11.4 - 645 pli | Average value: 24.8 kN/m Grade Count:768 |
| Peel Strength | 0.500 - 35.0 kN/m | 2.85 - 200 pli | Average value: 7.89 kN/m Grade Count:96 |
| Graves Tear Strength | 4.00 - 55.0 kN/m | 22.8 - 314 pli | Average value: 18.6 kN/m Grade Count:44 |
| Taber Abrasion, mg/1000 Cycles | 30.0 - 540 | 30.0 - 540 | Average value: 184 Grade Count:26 |
| Compression Set | 8.00 - 90.0 % | 8.00 - 90.0 % | Average value: 27.1 % Grade Count:564 |
| 16.0 - 95.0 % @Temperature 70.0 - 100 °C |
16.0 - 95.0 % @Temperature 158 - 212 °F |
Average value: 57.0 % Grade Count:147 | |
| 16.0 - 99.0 % @Temperature -25.0 - 158 °C |
16.0 - 99.0 % @Temperature -13.0 - 316 °F |
Average value: 57.0 % Grade Count:371 | |
| 16.0 - 99.0 % @Time 79200 - 605000 sec |
16.0 - 99.0 % @Time 22.0 - 168 hour |
Average value: 57.0 % Grade Count:371 | |
| Tensile Set | 33.0 - 95.0 % @Temperature 70.0 - 70.0 °C |
33.0 - 95.0 % @Temperature 158 - 158 °F |
Average value: 58.4 % Grade Count:15 |
| 33.0 - 95.0 % @Time 79200 - 79200 sec |
33.0 - 95.0 % @Time 22.0 - 22.0 hour |
Average value: 58.4 % Grade Count:15 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 50.0 - 170 °C | 122 - 338 °F | Average value: 93.4 °C Grade Count:212 |
| Minimum Service Temperature, Air | -60.0 - -30.0 °C | -76.0 - -22.0 °F | Average value: -48.2 °C Grade Count:241 |
| Brittleness Temperature | -65.0 - -21.0 °C | -85.0 - -5.80 °F | Average value: -59.2 °C Grade Count:41 |
| Flammability, UL94 | HB - V-0 | HB - V-0 | Grade Count:55 |
| Flame Spread | 37.0 - 54.0 mm/min | 1.46 - 2.13 in/min | Average value: 45.2 mm/min Grade Count:15 |
| Oxygen Index | 26.0 - 29.0 % | 26.0 - 29.0 % | Average value: 27.5 % Grade Count:8 |
| Ring & Ball Softening Point | 128 - 135 °C | 262 - 275 °F | Average value: 131 °C Grade Count:4 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 3.70 - 15.0 % | 3.70 - 15.0 % | Average value: 9.78 % Grade Count:21 |
| Transmission, Visible | 90.0 % | 90.0 % | Average value: 90.0 % Grade Count:67 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0100 - 1.00e+16 ohm-cm | 0.0100 - 1.00e+16 ohm-cm | Average value: 2.76e+15 ohm-cm Grade Count:79 |
| Surface Resistance | 10.0 - 9.90e+12 ohm | 10.0 - 9.90e+12 ohm | Average value: 5.55e+11 ohm Grade Count:10 |
| Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:5 |
| Dielectric Constant | 2.10 - 2.80 | 2.10 - 2.80 | Average value: 2.46 Grade Count:23 |
| Dielectric Strength | 24.0 - 50.0 kV/mm | 610 - 1270 kV/in | Average value: 29.9 kV/mm Grade Count:57 |
| Dissipation Factor | 0.000100 - 0.00510 | 0.000100 - 0.00510 | Average value: 0.00258 Grade Count:23 |
| Comparative Tracking Index | 550 - 600 V | 550 - 600 V | Average value: 564 V Grade Count:21 |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Butadiene Content | 60.0 - 78.0 % | 60.0 - 78.0 % | Average value: 70.2 % Grade Count:10 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 140 - 280 °C | 284 - 536 °F | Average value: 202 °C Grade Count:222 |
| Nozzle Temperature | 175 - 249 °C | 347 - 480 °F | Average value: 191 °C Grade Count:13 |
| Die Temperature | 140 - 249 °C | 284 - 480 °F | Average value: 198 °C Grade Count:130 |
| Melt Temperature | 140 - 280 °C | 284 - 536 °F | Average value: 197 °C Grade Count:347 |
| Head Temperature | 180 °C | 356 °F | Average value: 180 °C Grade Count:127 |
| Mold Temperature | 10.0 - 110 °C | 50.0 - 230 °F | Average value: 39.5 °C Grade Count:416 |
| Drying Temperature | 51.7 - 90.0 °C | 125 - 194 °F | Average value: 71.1 °C Grade Count:383 |
| Moisture Content | 0.0300 - 0.0400 % | 0.0300 - 0.0400 % | Average value: 0.0375 % Grade Count:24 |
| Dew Point | -17.8 °C | 0.000 °F | Average value: -17.8 °C Grade Count:5 |
| Injection Pressure | 1.38 - 124 MPa | 200 - 18000 psi | Average value: 60.4 MPa Grade Count:329 |