Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) Zytel® 73G30T NC010 is a 30% glass fiber reinforced, toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 115 H3.0 000000 Nylon 6-Copolymer, Glass Fiber Reinforced PA 6-Copolymer, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 130 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 130 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
conditioned; ISO 180-1U |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
Conditioned; ISO 180-1U |
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BKV 50 H2.0 EF DUS30 901510 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1U |
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 126F8 Nylon 6, 40% Glass Fiber SAXAMID 126F8 is a polyamide 6 injection-molding-grade reinforced with 40% glass fibers.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows hig.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6T3 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It shows its high mechanical strength over a long period and is able to perform at higher.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 180 |
Sax Polymers SAXLAC 340Q Acrylonitrile Butadiene Styrene Saxalac 340Q is an siliconized, UV protected, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tes.. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GB30 NL PBT, 30% glass bead reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR30 NL HS PA6.6, 30% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR30 NL HW PA6.6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NA40 GR35 NL HS PA6.6, 35% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 GR30 NL HW PA6, 30% glass fiber reinforced, hydrolysis stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecomid® NB40 GR25 NL PA6, 25% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® Nb40 GR30 NL PA6, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Sax Polymers SAXATEC 4115 Acrylonitrile Styrene Acrylate SAXATEC 4115 is a medium viscosity, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX .. |
|||
Izod Impact, Unnotched (ISO) | 80.0 kJ/m² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |