Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East) LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East) LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 180-1U |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Durethan® BKV 115 H2.0 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180-1U |
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180-1U |
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® V9280LW PET (Europe-Africa-Middle East) 40% Glassfiber / Mineral Filled PET, Impact Modifier, Mold Release, Heat StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 226F3 Nylon 6.6, 15% Glass Fiber SAXAMID 226F3 is a polyamide 6.6 injection-molding-grade reinforced with 15% glass fibers. This grade is suitable for applications requiring high strength and very good flow properties during proces.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East) NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GB20 NL PBT, 20% glass bead reinforced, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GR15 NL100 KA01 PBT/PET, 15% glass fiber reinforced, heat stabilized, natural, gas injection grade Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Eurotec® Tecodur® PB70 GR30 NL XA60 PBT, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus, heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NB30 GR15 BK005 FS90 PA6, 15% glass fiber reinforced, flame retardant - halogen & red phosphorus free, low smoke & toxic gas grade Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecomid® NB30 MF30 BK001 HS PA6, 30% mineral reinforced, heat stabilized, black Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
80x10x4; ISO 180/1U |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers |
|||
Izod Impact, Unnotched (ISO) | 35.0 kJ/m² @Temperature -40.0 °C |
16.7 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1U |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |