Mechanical Properties Metric English Comments
Tensile Modulus 6.00 GPa

@Temperature 150 °C
870 ksi

@Temperature 302 °F
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 6.00 GPa

@Temperature 90.0 °C
870 ksi

@Temperature 194 °F
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Carbon fiber. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma..
Tensile Modulus 6.00 GPa

@Temperature 23.0 °C
870 ksi

@Temperature 73.4 °F
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Modulus 6.00 GPa

@Temperature 150 °C
870 ksi

@Temperature 302 °F
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Carbon fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastic..
Tensile Modulus 6.00 GPa

@Temperature 150 °C
870 ksi

@Temperature 302 °F
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Modulus 6.00 GPa

@Temperature 120 °C
870 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. improved G.W.F.I. compared to standard product.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri..
Tensile Modulus 6.00 GPa

@Temperature 120 °C
870 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu..
Tensile Modulus 6.00 GPa

@Temperature 120 °C
870 ksi

@Temperature 248 °F
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInf..
Tensile Modulus 6.00 GPa

@Temperature 90.0 °C
870 ksi

@Temperature 194 °F
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 6.00 GPa

@Temperature 60.0 °C
870 ksi

@Temperature 140 °F
LATI Laril 13 G/20-V1 PPOm, 20% Glass Fiber Reinforced, Flame Retardant
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal..
Tensile Modulus 6.00 GPa

@Temperature 90.0 °C
870 ksi

@Temperature 194 °F
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced
Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; ..
Tensile Modulus 6.00 GPa

@Temperature 150 °C
870 ksi

@Temperature 302 °F
LATI Larton G/40 I6 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Good elongation. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa ..
Tensile Modulus 6.00 GPa

@Temperature 150 °C
870 ksi

@Temperature 302 °F
LATI Latamid 6 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Modulus 6.00 GPa

@Temperature 150 °C
870 ksi

@Temperature 302 °F
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced
Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: ..
Tensile Modulus 6.00 GPa

@Temperature 90.0 °C
870 ksi

@Temperature 194 °F
LATI Latigloss 62 H2 G/50 PA 6, 50% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 6 (PA6). Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Ameri..
Tensile Modulus 6.00 GPa

@Temperature 60.0 °C
870 ksi

@Temperature 140 °F
LATI Latilon 28D G/20-V0 PC, 20% Glass Fiber Reinforced, Flame Retardant
Polycarbonate (PC) based compound. Glass fibers. UL94 V-0 classified, brominated and chlorinated halogens-based flame retardants free. Low smoke density and low toxicity index. High dimensional stab..
Tensile Modulus 6.00 GPa

@Temperature 23.0 °C
870 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66
Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 6.00 GPa

@Temperature 177 °C
870 ksi

@Temperature 351 °F
IM7 (12K); [90°]16; Wet Condition
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form
Fiber: T300-12K, IM7-12KInformation provided by HexCel
Tensile Modulus 6.00 GPa

@Temperature 90.0 °C
870 ksi

@Temperature 194 °F
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced
Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI..
Tensile Modulus 6.00 GPa

@Temperature -40.0 °C
870 ksi

@Temperature -40.0 °F
ISO 527
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..