Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Flexural Yield Strength | 79.4 MPa | 11500 psi | DIN 53455; ASTM D790 |
Kolon SPESIN® KP513FLBL Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Yield Strength | 79.4 MPa | 11500 psi | ASTM D790 |
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Flexural Yield Strength | 79.3 - 160 MPa | 11500 - 23200 psi | Average value: 104 MPa Grade Count:9 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Flexural Yield Strength | 79.0 - 83.0 MPa | 11500 - 12000 psi | Average value: 80.5 MPa Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 79.4 MPa @Thickness 3.20 mm |
11500 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Flexural Yield Strength | 79.4 MPa @Thickness 3.20 mm |
11500 psi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000W PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Flexural Yield Strength | 79.4 MPa @Thickness 3.20 mm |
11500 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific) LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc.. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES HiFill® PP GF/M40 CC BK 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 79.4 MPa | 11500 psi | ASTM D790 |
Samyang Triloy® 220 Polymer Alloy, High Impact Excellent impact, formability and weather resistance.220 is a high impact grade.Applications: Automotive instrument panels and knob typesInformation provided by Samyang. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP.. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES Electrablend® ABS SS10 FR BK 10% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackInformation pr.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® V3802 PBT + PC + PET (Asia Pacific) PBT + PC + PET, Mold Release, Flame retardant, Impact Modified, OpaqueThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Techmer ES HiFill® PP GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 79.3 MPa | 11500 psi | ASTM D790 |
Devcon High-Performance Backing Compound Epoxy Abrasion-Resistant SystemData provided by Ellsworth Adhesives. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
Chem Polymer Durlex 700 PBT, General Purpose A lubricated, general purpose PBT.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Flexural Yield Strength | 79.3 - 310 MPa @Temperature -40.0 - 150 °C |
11500 - 45000 psi @Temperature -40.0 - 302 °F |
Average value: 176 MPa Grade Count:1 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |