Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 88.3 MPa | 12800 psi | DIN 53455; ASTM D790 |
Kolon SPESIN® KP210 General Purpose PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
1mm/min; ASTM D790 |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | DIN 53455; ASTM D790 |
Kolon KOPA® KN333HI2 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | DIN 53455; ASTM D790 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
KEP Kepital® F10 Standard Grade/High Viscosity Acetal Homopolymer Extrusion: electrical parts, machine/mechanical parts, industrial parts, automotive parts, applications, electronic data processing parts, thick-walledKepital® is a registered trademark of Korea .. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti.. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000GU PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Info.. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
5mm/min; ASTM D790 |
LG Chemical Lupox® TE5000SZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 137050-02-03, 26062-94-2 and 103598-77-2Information provided by LG Chemical |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SC1004L PC, High Impact Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3017PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3020PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020PJ is a high flow grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3020U UV Stable Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020U is a high flow, UV Stable grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3022PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022PJ is a general use grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3022R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022R is a general use grade with heat stabilizers and separating materials added.Appli.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3025PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025PJ is a general use grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3025R Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025R is a general use grade with heat stabilizers and separating materials added.Appli.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3027PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PJ is an extrusion grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3027PU(X) Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PU(X) is an extrusion grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Samyang Trirex® 3030IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® D202 PBT, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Cheng Yu Plastic PP236G1 Polypropylene, 10% Glass Fiber |
|||
Flexural Yield Strength | 88.3 MPa | 12800 psi | ASTM D790 |
Cheng Yu Plastic VH826 Flame Retardant ABS, Medium Impact |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IMC-45V ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 6.40 mm |
12800 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMG1120 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Flexural Yield Strength | 88.3 MPa @Thickness 3.20 mm |
12800 psi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY SC1004ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical.. |