Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94 ABS Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East) PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Flexural Yield Strength | 79.0 - 83.0 MPa | 11500 - 12000 psi | Average value: 80.5 MPa Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2 mm/min; ISO 178 |
LG Chemical HT-700 ABS, High Strength, High Scratch Resistance Information Provided by LG Chem |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP GL003 PSU (Asia Pacific) LNP* Lubricomp* GL003 is a compound based on Polysulfone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX NX0031 PPE+PA NORYL GTX* NX0031 resin is a conductive resin specially designed for electrostatic painting and powder coating applications. This material combines high impact, good flow and conductivity. The mate.. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® V3802 PBT + PC + PET (Asia Pacific) PBT + PC + PET, Mold Release, Flame retardant, Impact Modified, OpaqueThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 5E003M FP-V (PVDF) LNP* THERMOCOMP* 5E003M is a compound based on PVDF resin containing 15% Milled Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific) This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
Chem Polymer Durlex 700 PBT, General Purpose A lubricated, general purpose PBT.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/02T Acetal - 2% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | ASTM D790 |
PolyOne Lubri-Tech™ MP-000/10T Modified PPO - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Flexural Yield Strength | 79.0 MPa | 11500 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |