Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.60 GPa | 812 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers Nemcon™ E PC 08CF Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments where strict control of ESD and cleanliness are critical. Nemcon E PC 08CF is a carbon fiber-reinforced polyca.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | conditioned, 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® AKV 30 G HR DUS023 900116 Nylon 66, 30% Glass Fiber PA 66, 30% glass fiber, injection molding, improved flowability, hydrolysis stabilized, improved surface finish, GIT/WITInformation provided by LANXESS. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Durethan® BKV 115 DUS008 000000 Nylon 6, 15% Glass Fiber PA 6, 15% glass fibers, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 330 H2.0 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding type, 30% glass fibers, branched/structural viscosity, good weldability (vibration or hot plate), good heat-ageing resistance |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | |
LATI Latilub 73/13-15T G/15 POM, 15% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MFB44S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFB44S is a compound based on Polypropylene resin containing Glass Fiber, Glass Beads. Added features include; Heat Stabilized, Cu-Stabilized. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527 |
Polyram Polytron P30N03 Polypropylene, 30% Long Glass Fibers A chemically coupled 30% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance chara.. |
|||
Tensile Modulus | 5.60 GPa @Temperature 180 °C |
812 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-25/4 PA666-GF25 Information provided by EMS Grivory |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 LF 15/1 PA666-(GF+Z)45 Information provided by EMS Grivory |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1 mm/min; ISO 527 |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 XEC1 POM Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe .. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS BK-102 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature performance and d.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ASTM D638 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Conditioned) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Europe-Africa-Middle East) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | |
LATI Latigea B02 H6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Improved thermal stability. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 5.60 GPa | 812 ksi | ISO 527-1/-2 |
Lanxess Pocan® DP 7102 000000 PBT, 30% Mineral
(discontinued **) PBT, 30% mineral, injection molding, LDS |