Mechanical Properties Metric English Comments
Tensile Modulus 4.70 GPa
682 ksi
Plastcom SLOVAMID 66 GB 30 LS PA66, 30% glass beads, light stability
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C4210HF is a 10% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low sh..
Tensile Modulus 4.70 GPa
682 ksi
ISO 527
Nilit FRIANYL A63 W-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Modulus 4.70 GPa

@Thickness 4.00 mm,
Temperature 23.0 °C
682 ksi

@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2
PolyOne Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Tensile Modulus 4.70 GPa
682 ksi
STN EN ISO 527-2
Plastcom SLOVALEN PH 49 GF 20 Polypropylene Homopolymer, 20% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fiber, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP..
Tensile Modulus 4.70 GPa
682 ksi
conditioned, 1 mm/min; ISO 527-1,-2
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber
PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS.
Tensile Modulus 4.70 GPa
682 ksi
Conditioned; ISO 527-1/-2
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber
PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance
Tensile Modulus 4.70 GPa
682 ksi
ISO 527-1/-2
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber
PBT, 7% glass fibers, injection molding, flame retardant
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL V02570 PPE+HIPS
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Tensile Modulus 4.70 GPa
682 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East)
VALOX 4012 is a 10% high strength glass fibre reinforced PBT injection moulding resin with improved mechanical properties. Applications: connectors.
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East)
VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics.
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp GX05053 PSU (Europe-Africa-Middle East)
LNP* THERMOCOMP* GX05053 is a compound based on Polysulfone blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp MF004S PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF004S is a compound based on Polypropylene resin, containing Glass Fiber. Added features include; Chemically Coupled.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Tensile Modulus 4.70 GPa

@Temperature 180 °C
682 ksi

@Temperature 356 °F
ISO 527-1/-2
DSM Stanyl® 46HF4530 PA46-GF30
30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications
Tensile Modulus 4.70 GPa
682 ksi
50mm/min; ISO 527-1
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Tensile Modulus 4.70 GPa
682 ksi
50mm/min; ISO 527-1
Denka TP-801 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Tensile Modulus 4.70 GPa
682 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p..
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
Eurostar Starflam PK00032E PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Starflam PK0032E is a Halogen Free Red Phosphorous Free Flame Retardant Mineral Filled Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Tensile Modulus 4.70 GPa
682 ksi
ISO 527-1
Barlog Plastics KEBAFORM C 8027 POM Copolymer, 30% mineral reinforced
POM-MD30Information provided by BARLOG plastics GmbH.
Tensile Modulus 4.70 GPa
682 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOTUF WF003I PBT (Europe-Africa-Middle East)
LNP* Thermotuf* WF003I BLACK is a compound based on Polybutylene Terephalate resin containing Glass Fiber. Added features of this material include: High Impact.