Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.50 GPa | 508 ksi | STN EN ISO 527-2 |
Plastcom PLASTAMID® 66 BT B 27 TS PA66 heat stabilized Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - elec.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Nilit FRIANYL B63 KG30 Nylon 6 for injection molding, 30% chalk filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527-1/2 |
Radici Radiflam® AFR (dry) Nylon 66 PA66 Self-extinguishing without halogens or phosphorousInformation provided by Radici group. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Nilit FRIANYL A63 V0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ASTM D638 |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 7375 000000 PBT, White Pigment PBT, 25% white pigments, injection molding, improved light reflection, low tendency to warp |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | |
LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | |
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 (Asia Pacific) LNP* Lubricomp* RAL22S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Asia Pacific) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Styron CALIBREâ„¢ 7102-8 Polycarbonate CALIBREâ„¢ 7102-8 glass-reinforced resin offers increased modulus and improved heat distortion resistance, with minimal shrinkage. It also offers outstanding UL-94 flammability ratings. CALIBRE.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6
(Unverified Data**) 15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
Eurotec® Tecomid® NA30 NL RM PA6.6, MoS2 modified, natural Information provided by Eurotec® |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.50 GPa | 508 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |