| Category | Polymer , Thermoplastic |
| Manufacturer | Wolf Kunststoff |
| Trade Name | ZEDEX® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.51 g/cc | 0.0546 lb/in³ | ISO 1183 |
| Water Absorption | 0.010 % @Temperature 23.0 °C |
0.010 % @Temperature 73.4 °F |
RMC 93%; DIN EN ISO 62 |
| Moisture Absorption at Equilibrium | 0.050 % | 0.050 % | DIN EN ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 100 | >= 100 | DIN 53505 |
| Hardness, Shore D | 83 | 83 | DIN 53505 |
| Ball Indentation Hardness | 134 MPa | 19400 psi | DIN 2039 |
| Tensile Strength at Break | 50.0 MPa | 7250 psi | DIN EN ISO 527 |
| Tensile Strength | 50.0 MPa | 7250 psi | DIN EN ISO 527 |
| Tensile Stress | 19.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
2760 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | Elastic Limit |
| Elongation at Break | 4.5 % | 4.5 % | Flexural; DIN EN ISO 178 |
| 4.5 % | 4.5 % | DIN EN ISO 527 | |
| Elongation at Yield | 1.3 % | 1.3 % | Elastic Yield Point |
| 4.5 % | 4.5 % | Elongation at Maximum Force; DIN EN ISO 527 | |
| 4.9 % | 4.9 % | Flexural; DIN EN ISO 178 | |
| Tensile Modulus | 3.50 GPa | 508 ksi | DIN EN ISO 527 |
| Flexural Strength | 74.0 MPa | 10700 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
| 80.0 MPa | 11600 psi | DIN EN ISO 178 | |
| 81.0 MPa | 11700 psi | DIN EN ISO 178 | |
| Flexural Modulus | 3.00 GPa | 435 ksi | DIN EN ISO 178 |
| Compressive Yield Strength | 109 MPa | 15800 psi | DIN EN ISO 604 |
| Compressive Strength | 71.0 MPa | 10300 psi | Elastic Limit |
| 92.0 MPa | 13300 psi | break; DIN EN ISO 604 | |
| 109 MPa | 15800 psi | DIN EN ISO 604 | |
| 25.0 MPa @Time 3.60e+7 sec |
3630 psi @Time 10000 hour |
||
| 37.0 MPa @Time 360000 sec |
5370 psi @Time 100 hour |
||
| 76.0 MPa @Time 36.0 sec |
11000 psi @Time 0.0100 hour |
||
| 29.0 MPa @Strain 3.50 % |
4210 psi @Strain 3.50 % |
DIN EN ISO 604 | |
| Compressive Modulus | 3.50 GPa | 508 ksi | DIN EN ISO 604 |
| Fatigue Strength | 40.0 MPa @# of Cycles 1.00e+6 |
5800 psi @# of Cycles 1.00e+6 |
1 Hz |
| K Factor (ISO) | 0.50 µm/km @Temperature 20.0 °C |
0.50 µm/km @Temperature 68.0 °F |
|
| 1.1 µm/km @Temperature 100 °C |
1.1 µm/km @Temperature 212 °F |
||
| 3.3 µm/km @Temperature 200 °C |
3.3 µm/km @Temperature 392 °F |
||
| 4.2 µm/km @Temperature 240 °C |
4.2 µm/km @Temperature 464 °F |
||
| Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | EN ISO 179/1eU |
| Charpy Impact, Notched | 0.917 J/cm² | 4.36 ft-lb/in² | EN ISO 179/1eA |
| Coefficient of Friction, Dynamic | 0.11 @Temperature 100 °C |
0.11 @Temperature 212 °F |
Dry Operation |
| 0.17 @Temperature 20.0 °C |
0.17 @Temperature 68.0 °F |
Dry Operation | |
| Coefficient of Friction, Static | 0.18 @Temperature 20.0 °C |
0.18 @Temperature 68.0 °F |
Dry Operation |
| Tensile Creep Modulus, 1000 hours | 1900 MPa | 276000 psi | At 1% Deformation; DIN 53444 |
| Limiting Pressure Velocity | 0.400 MPa-m/sec | 11400 psi-ft/min | v = 200m/min |
| 0.624 MPa-m/sec | 17800 psi-ft/min | v = 1m/min | |
| 0.66666 MPa-m/sec | 19033 psi-ft/min | v = 100m/min | |
| 1.26 MPa-m/sec | 36000 psi-ft/min | v = 10m/min | |
| Compression Set | 6.5 % | 6.5 % | |
| 11 % | 11 % | Nominal Compressive Strain at Break; DIN EN ISO 604 | |
| 31 % | 31 % | Nominal Compressive Strain at Compressive Strength; DIN EN ISO 604 | |
| 31 % | 31 % | Nominal Compressive Yield Strain; DIN EN ISO 604 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 60.0 µm/m-°C @Temperature <=100 °C |
33.3 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
| 90.0 µm/m-°C @Temperature <=150 °C |
50.0 µin/in-°F @Temperature <=302 °F |
ISO E 831 | |
| Specific Heat Capacity | 0.890 J/g-°C | 0.213 BTU/lb-°F | DSC |
| Melting Point | 320 °C | 608 °F | DSC |
| Maximum Service Temperature, Air | 90.0 °C | 194 °F | Pressed Bushings |
| 240 °C | 464 °F | Continuous | |
| 290 °C | 554 °F | Short Term (3h) | |
| Deflection Temperature at 1.8 MPa (264 psi) | 135 °C | 275 °F | DIN EN ISO 75 |
| Glass Transition Temp, Tg | 110 °C | 230 °F | DSC |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | 47 % | 47 % | DIN EN ISO 4589 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 4.50e+16 ohm-cm | 4.50e+16 ohm-cm | IEC 93 |
| Surface Resistance | 4.40e+16 ohm | 4.40e+16 ohm | IEC 93 |
| Dielectric Constant | 4.1 @Frequency 110 Hz |
4.1 @Frequency 110 Hz |
IEC 250 |
| Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 243 |
| Dissipation Factor | 0.020 | 0.020 | IEC 112 |
| 0.055 @Frequency 1.00 Hz |
0.055 @Frequency 1.00 Hz |
||
| Comparative Tracking Index | 130 V | 130 V | IEC 112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Alignment Adjustment | 2 | Nominal Scale: 1, low; 10, high |
| Chemical Sterilization | 10 | Nominal Scale: 1, low; 10, high |
| Color | Beige | |
| Creep Resistance | 4 | Nominal Scale: 1, low; 10, high |
| Dimensional Stability with Thermal Expansion | 4 | Nominal Scale: 1, low; 10, high |
| FDA Compliant | Applicable | |
| Free from Silicon | Applicable | |
| Gamma-rays Radiation Sterilization | 4 | Nominal Scale: 1, low; 10, high |
| High Precision Bushings (negative clearance) | Applicable | |
| Injection Molded Parts | Applicable | |
| Machined Parts | Applicable | |
| Moist Heat Sterilization | 7 | Nominal Scale: 1, low; 10, high |
| Plastic Granules | Applicable | |
| Rate of Desorption | 2.8E-07 | a = .44 |
| Resistance Against dust, Dirt, Abrasive Substances | 6 | Nominal Scale: 1, low; 10, high |
| Resistance Against Hot Water | 140 | |
| Resistance to Chemicals | 10 | Nominal Scale: 1, low; 10, high |
| Resistant Against Disinfectant | Applicable | |
| Rods up to Øe (de) | Applicable | |
| ROHS/WEEE | Applicable | |
| Sheets up to Maximum Thickness | Applicable | |
| Sliding Velocity | 300 | |
| Suitable for Outdoor Use | 7 | Nominal Scale: 1, low; 10, high |
| Suitable for Use in Water | Applicable | |
| Suitable for Vacuum | Applicable | |
| UV Rays Resistance | 8 | Nominal Scale: 1, low; 10, high |
| UV-Sterilization | 7 | Nominal Scale: 1, low; 10, high |