Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.10 GPa | 450 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 41 GF 10 Polypropylene Homopolymer, 10% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Tensile Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® SC655 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® SC655 is a medium viscosity acetal homopolymer, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 2505 000000 PBT PBT, non-reinforced, injection molding, flame retardant |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | |
LATI Latiblend 3675 G/10 ABS/PBT, 10% Glass Fiber Reinforced Blend based on Acrylonitrile-Butadiene-Styrene copolymer (ABS) / Polybutylene Terephthalate (PBT). Glass fibers. Good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ASTM D638 |
Spartech Polycast UVT (Ultra-Violet Transmitting) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Tensile Modulus | >= 3.10 GPa @Temperature 23.9 °C |
>= 450 ksi @Temperature 75.0 °F |
|
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ASTM D638 |
Westlake Plastics Corzan® II CPVC Sheet Corzan® II CPVC, manufactured from Corzan G2 resin, was developed for use in the construction of wet benches and other cleanroom equipment for the semiconductor industry. It meets Factory Mutual.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 3010N 5-SL4-3X NAT PA66 FR Low Viscosity, Molding Release, 30% Glass Reinforced |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8202 HS BK-102 PA6 (Dry) Ultramid 8202 HS BK-102 is an unfilled, heat stabilized, pigmented black, low viscosity, general purpose injection molding PA6 exhibiting excellent fluidity for filling thin sections. It possesses .. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac®-C HC450 Copolymer Acetal Resin New Copolymer, the improvement of physical properties of standard gradesInformation provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, DAM Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||
Tensile Modulus | 3.10 GPa | 450 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB009 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productiv.. |
|||
Tensile Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
Tensile Modulus | >= 3.10 GPa | >= 450 ksi | |
Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding .. |