Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced , Epoxy, High Temperature
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond EP42HT-2LO Low Outgassing, Heat Resistant Two Component Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Master Bond Polymer System EP42HT-2LO is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along with outstanding chemical resistance. EP42HT-2LO is a superior epoxy adhesive system and is castable to thicknesses exceeding 2-3 inches. EP42HT-2LO cures readily at ambient temperatures or more quickly at elevated temperatures. One particularly popular cure schedule is overnight at room temperature followed by 2-4 hours at 150-200°F. EP42HT-2LO has excellent physical strength properties and dimensional stability. It is suitable for cryogenic service down to 4K.
Physical Properties Metric English Comments
Viscosity 30 - 70 cP

@Temperature 23.9 °C
30 - 70 cP

@Temperature 75.0 °F
Part B
1000 - 1800 cP

@Temperature 52.0 °C
1000 - 1800 cP

@Temperature 126 °F
Part A
55000 - 110000 cP

@Temperature 23.9 °C
55000 - 110000 cP

@Temperature 75.0 °F
Part A
Mechanical Properties Metric English Comments
Hardness, Shore D >= 75
>= 75
Tensile Strength >= 82.7 MPa
>= 12000 psi
Elongation at Break <= 5.0 %
<= 5.0 %
Tensile Modulus >= 3.10 GPa
>= 450 ksi
Shear Strength >= 13.8 MPa
>= 2000 psi
Tensile lap, Al/Al
Thermal Properties Metric English Comments
CTE, linear 35.0 - 40.0 µm/m-°C
19.4 - 22.2 µin/in-°F
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -269 °C
-452 °F
Optical Properties Metric English Comments
Refractive Index 1.62
1.62
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
Dielectric Constant 3.8

@Frequency 60.0 Hz
3.8

@Frequency 60.0 Hz
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 100 °C
2.00 - 3.00 hour

@Temperature 212 °F
2880 - 4320 min

@Temperature 23.9 °C
48.0 - 72.0 hour

@Temperature 75.0 °F
Pot Life 45 - 75 min
45 - 75 min
100 gram batch
Shelf Life 12.0 Month
12.0 Month
in original unopened containers
Descriptive Properties Value Comments
Mixing Ratio (A to B) 100:40
by weight, Part A to Part B
100:50
by volume, Part A to Part B