Material Notes:
Delrin® SC655 is a medium viscosity acetal homopolymer, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa

@Temperature 23.0 °C
10200 psi

@Temperature 73.4 °F
ISO 527
Elongation at Yield 17 %

@Temperature 23.0 °C
17 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Appearance Natural Color
Features Creep Resistance, Good
Dimensional Stability, Good
Fatigue Resistant
Homopolymer
Impact Resistance, Good
Stiffness, High
Strength, High
Viscosity, Medium
Forms Pellets
Generic Acetal (POM) Homopolymer
Material Status Current
Part Marking Code >POM<
ISO 11469
Processing Method Extrusion
Injection Molding
Product Category Healthcare Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification POM
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Fasteners
Gears
General Purpose
Medical Applications
Parts, Engineering