Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Plaskolite Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific) CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Quadrant EPP Acetron® AF Blend POM-H Acetal Extruded PTFE-Filled Acetal Homopolymer (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
FKuR Kunststoff Biograde® C 7500 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | |
LATI Latishield 73/13-07A POM, Steel Fiber Reinforced EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | |
LATI Latistat 73/13-06 POM Dissipative product based on Polyoxymethylene (POM). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | DIN 53457 |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 226 Nylon 6.6 SAXAMID 226 is a general purpose polyamide 6.6 injection-molding-grade. Benefits are short cycle times and good release properties.Information provided by SAX Polymers |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
Unitika A1022GFL15 PA6, 15% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
Unitika A125 PA66, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527; DIN 53452 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 CP Nylon 6, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® FG 34 NL nat 6023 PA6 Product description: Grilon FG 34 NL natural 6023 is a modified, medium viscosity polyamide 6. Grilon FG 34 NL natural 6023 exhibits following improvements compared to a PA 6: Better gas barrier pro.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® GTR 45 PA6I/6T Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing .. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG50 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436W40L1 Wollastonite Reinforced |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Ascend Performance Materials Vydyne® 66B, 66J Nylon 66, Dry as Molded Vydyne® 66B and 66J are members of a family of unreinforced extrusion grade Nylon 66 resins. They are available in natural color. These resins offer high strength, rigidity, and toughness for a bro.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | 1mm/min; ISO 527 |
BASF Ultramid® B50L 01 PA6 (Dry) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ASTM Test |
BASF Ultramid® B27 E 01 PA6 (Dry) Ultramid B27 E 01 is a low viscosity general-purpose, extrusion PA6 grade well suited for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® G 16 PA6I/6T Product description: Grivory G 16 is a low viscosity amorphous copolyamide. It is suitable for injection - stretch blow molding, injection blow molding, extrusion blow molding, the manufacture of co.. |
|||
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® SC652 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® SC652 is a medium viscosity acetal homopolymer, with an advanced system of lubricants. It is developed for parts requiring low wear, low friction and low squeak noise for the healthcare ind.. |
|||
Tensile Modulus | 3.00 GPa | 435 ksi | ISO 527 |
BASF Ultramid® A3K Q601 PA66(Dry) Description: Ultramid A3K Q601 is an easy flowing, injection molding grade PA66.Applications: Typical applications include fast processing high stress technical parts or electrically insulating part.. |