North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Wood Filled
Manufacturer North Wood Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It is made with only the highest quality recycled resins. 2:1 Polypropylene:UNIFILL-60 yields an end product with 20% fiber.
Physical Properties Metric English Comments
Density 0.978 g/cc
0.0353 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0092 cm/cm
0.0092 in/in
ASTM D955
Melt Flow 1.3 g/10 min

@Temperature 190 °C
1.3 g/10 min

@Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 4.1 %
4.1 %
ASTM D638
Tensile Modulus 3.00 GPa
435 ksi
ASTM D638
Flexural Yield Strength 38.0 MPa
5510 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.220 J/cm
0.412 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.20 J/cm
2.25 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature <= 200 °C
<= 392 °F
To prevent fiber degradation.