Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® GTR 45 PA6I/6T

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® GTR 45 PA6I/6T.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides the most interesting property of Grivory GTR 45 is the transparency even at high wall thicknesses. Grivory GTR 45 is suitable for production of optically and technically demanding parts in the application segments: Electro / ElectronicsMechanical engineeringDomestic appliancesSafety technologyPackaging Grivory GTR 45 can be used where transparency with solvent resistance is needed and is particularly suitable and approved for parts in contact with non alcoholic food, cosmetics and cold ( < 30°C) drinking water.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 145 MPa
21000 psi
dry; ISO 2039-1
145 MPa
21000 psi
conditioned; ISO 2039-1
Tensile Strength, Yield 100 MPa
14500 psi
conditioned; ISO 527-1/-2
100 MPa
14500 psi
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
conditioned; ISO 527-1/-2
<= 50 %
<= 50 %
dry; ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
conditioned; ISO 527-1/-2
5.0 %
5.0 %
dry; ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
conditioned; ISO 527-1/-2
3.00 GPa
435 ksi
dry; ISO 527-1/-2
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179/1eA
0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
0.200 J/cm²

@Temperature 30.0 °C
0.952 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
Maximum Service Temperature, Air 40.0 - 60.0 °C
104 - 140 °F
long term; EMS
70.0 °C
158 °F
short term; EMS
Transformation Temperature, Tg 125 °C
257 °F
10°C/min; ISO 11357-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ISO 75-1/-2
Flammability, UL94 V-2
V-2
IEC 60695-11-10
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
dry; IEC 60243-1
27.0 kV/mm
686 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Electricals & Electronics Electrical appliances
Food contact EU Requirements
FDA
Form Granules
Industry & Consumer goods Housewares
Medical USP VI
Packaging Cosmetics / Personal care
Injectionstretchblowmoulded containers
Medical packaging
Processing Injection (stretch) blow molding
Injection Molding
Product Attributes Barrier Properties
Partially aromatic Polyamide
Special Characteristics Transparent
Users viewing this material also viewed the following: