Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AR is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ares colour effects. The colour package may effect performance.This data was supplie.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East) CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
LG Chemical HI-151 ABS, Middle Impact Information Provided by LG Chem |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | |
Ineos ABS Lustran® H604 Standard impact strength.,Property data per ISO test methods. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP SG004 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SG004 is a compound based on PA 12 resin containing Graphite. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1mm/min; ISO 527 |
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin Thin-wall injection moldings grade of high fluidity. It has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Comparatively large-size components of mechanic.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1mm/min; ISO 527 |
Teijin Panlite® L-1250Z100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is an injection molding grade that has normal fluidity and weather resistance and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, elect.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527 |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East) NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX HX7409HP PC+POLYESTER Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Covestro Apec® 1895 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=183 °CPreprocessingMax. Water content |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ASTM D638 |
Covestro Makrolon® 3258 Polycarbonate, General Purpose, Mold Release, Biocompatibility It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 40 HWCP 40% Glass Sphere Filled Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BT 40 Z PA6 Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Covestro Makrolon® Rx2530 Polycarbonate ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 .. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ASTM D638 |
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | |
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
Lanxess Pocan® S 7020 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |