Material Notes:
Information Provided by LG Chem
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ISO 2577
Melt Index of Compound 24.15 g/10 min

@Load 10.0 kg,
Temperature 220 °C
24.15 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
50 mm/min; ISO 527
Elongation at Break 15 %
15 %
50 mm/min; ISO 527
Elongation at Yield 5.0 %
5.0 %
50 mm/min; ISO 527
Tensile Modulus 2.40 GPa
348 ksi
1 mm/min; ISO 527
Flexural Yield Strength 77.0 MPa
11200 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
ISO 180
22.0 kJ/m²

@Temperature 23.0 °C
10.5 ft-lb/in²

@Temperature 73.4 °F
ISO 80
Charpy Impact Unnotched 7.00 J/cm²

@Temperature -30.0 °C
33.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179
8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
ISO 179
2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °C
207 °F
Annealed, 80°C, 4 hours; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
Annealed, 80°C, 4 hours; ISO 175
Vicat Softening Point 96.0 °C
205 °F
50 N, 50°C/h; ISO 306
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 220 - 250 °C
428 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 75.0 - 85.0 °C
167 - 185 °F
Dry Time 2 - 4 hour
2 - 4 hour
Predrying
Users viewing this material also viewed the following: