| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded |
| Manufacturer | Covestro |
| Trade Name | Apec® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Covestro Apec® 1800 Polycarbonate.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
| 0.980 g/cc <br>@Temperature 330 °C |
0.0354 lb/in³ <br>@Temperature 626 °F |
Melt | |
| Water Absorption | 0.30 % | 0.30 % | Similar to ISO 62 |
| Moisture Absorption at Equilibrium | 0.12 % | 0.12 % | Similar to ISO 62 |
| Melt Flow | 10 g/10 min <br>@Load 2.16 kg,<br> Temperature 330 °C |
10 g/10 min <br>@Load 4.76 lb,<br> Temperature 626 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
| Elongation at Break | >= 50 % | >= 50 % | Nominal; ISO 527-1/-2 |
| Elongation at Yield | 6.8 % | 6.8 % | ISO 527-1/-2 |
| Tensile Modulus | 2.40 GPa | 348 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | NB | NB | ISO 179/1eU |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
ISO 179/1eU | |
| Impact | 5500 | 5500 | Puncture - maximum force (N); ISO 6603-2 |
| 6400 <br>@Temperature -30.0 °C |
6400 <br>@Temperature -22.0 °F |
Puncture - maximum force (N); ISO 6603-2 | |
| Puncture Energy | 60.0 J | 44.3 ft-lb | ISO 6603-2 |
| 65.0 J <br>@Temperature -30.0 °C |
47.9 ft-lb <br>@Temperature -22.0 °F |
ISO 6603-2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C | 38.9 µin/in-°F | ISO 11359-1/-2 |
| Specific Heat Capacity | 1.70 J/g-°C | 0.406 BTU/lb-°F | Melt |
| Thermal Conductivity | 0.167 W/m-K | 1.16 BTU-in/hr-ft²-°F | Melt |
| Deflection Temperature at 0.46 MPa (66 psi) | 174 °C | 345 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 159 °C | 318 °F | ISO 75-1/-2 |
| Flammability, UL94 | HB <br>@Thickness 1.50 mm |
HB <br>@Thickness 0.0591 in |
IEC 60695-11-10 |
| Oxygen Index | 25 % | 25 % | ISO 4589-1/-2 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 80 % | 80 % | transparent; thickness unknown |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | IEC 60093 |
| Dielectric Constant | 3.0 <br>@Frequency 100 Hz |
3.0 <br>@Frequency 100 Hz |
IEC 60250 |
| 3.0 <br>@Frequency 1.00e+6 Hz |
3.0 <br>@Frequency 1.00e+6 Hz |
IEC 60250 | |
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.00070 <br>@Frequency 100 Hz |
0.00070 <br>@Frequency 100 Hz |
IEC 60250 |
| 0.0080 <br>@Frequency 1.00e+6 Hz |
0.0080 <br>@Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 330 °C | 626 °F | Injection Molding; ISO 294 |
| 330 - 340 °C | 626 - 644 °F | ||
| Mold Temperature | 100 °C | 212 °F | Injection Molding; ISO 10724 |
| 120 - 140 °C | 248 - 284 °F | ||
| Ejection Temperature | 165 °C | 329 °F | |
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Availability | Europe | |
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Eff. thermal diffusivity (m²/s) | 1E-07 | |
| Form | Pellets | |
| Process | Film Extrusion | |
| Injection Molding | ||
| Profile Extrusion | ||
| Sheet Extrusion |