Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.06 GPa | 299 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® X11 ABS Automotive: High heat resistance. Excellent flow/impact balance. UL94 HB rated. High gloss. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific) LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Asia Pacific) LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa @Thickness 3.20 mm |
299 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
Tensile Modulus | 2.06 GPa @Thickness 3.20 mm |
299 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical LI968W Co-Extrusion ASA Description: Good WeatherabilityApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC LNP* LUBRICOMP* DX98306H is a compound based on Polycarbonate resin containing Proprietary Fillers. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific) LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly LNP* LUBRICOMP* KP004L is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific) LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030 |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing... |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRILOY K2000XXH Acetal LNP LUBRILOY* K2000XXH is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material are: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® VH-0819 ABS, Unreinforced FR Flame-retardant high flow ABS that can be used for the exterior of large TV and OA devicesInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® HI-1001BN PC/ABS, Unreinforced PC/ABS that is used for the housing of mobile phone, wheel cap, rice cooker, electric iron etc., refrigerator door handle, panel etc.Information provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | Storage |
Epoxy Technology EPO-TEK® 301-2 Optically Transparent Epoxy Product Description: EPO-TEK® 301-2 is a two component optical, medical, and semiconductor grade epoxy resin, with low viscosity, long pot-life, and good handling characteristics.Advantages & Appli.. |
|||
Tensile Modulus | 2.06 GPa | 299 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific) LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |