Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527 |
Nilit FRIANYL B63 BR90 Nylon 6.6 for injection molding, 90% bronze filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MB006SXP PP (Europe-Africa-Middle East) LNP* Thermocomp* MB006SXP is a compound based on Polypropylene resin containing Glass Bead. Added featurs include: Heat Stabilized. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East) LNP* LUBRICOMP* IP004Z is a compound based on PA 6/12 resin containing PTFE, Silicone. Added features include : Internally Lubricated, Extrusion grade. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM-D790 |
Polyram RamShine PAS100 ASA, General Purpose General purpose injection molding ASAInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Goodfellow TPX® DX845 Extrusion Grade Polymethylpentene This grade is highly recommended for film extrusion; also for injection molding, fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensiv.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Goodfellow TPX® RT31 Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Eastman Aspira EB062 Copolyester Resin for Extrusion Blown Bottles Applications:Beverage packagingBottlesExtrusion blow moldingFood packagingPersonal care bottlesKey Attributes:Easy to extrude, cut, print and sealEffective barrier propertiesExcellent chemical resis.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | Tangent, MD; ASTM D882 |
Eastman Sahara Film Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BKZ-30 PA6-GB30 Information provided by EMS Grivory |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 MR 209 HWCP 20% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | Secant; ISO 527-2/50 |
ExxonMobil Exxtral™ CMU 101 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for automotive interior trim in which good surface finish, high scratch resistance and good UV resistance are required.Availa.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | 1.90 GPa @Temperature 23.0 °C |
276 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 41308 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 41308/0001 PVDF is specifically developed for coextrusion.Information provided by Solvay Specialty Polymers. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 55 LY PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c.. |
|||
Tensile Modulus | 1.90 GPa | 276 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, Conditioned Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, .. |