Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Premix Premi-Glas® 2550® AM CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® AM CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generati.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Premix Premi-Glas® 2550® CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas 2550® CR-SX is an advanced fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications where stringent flame spread and smoke generation .. |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B70 W25 G45 H Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527 |
Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade
(discontinued **) Contains PTFE lubricant. Used for injection molding of high performance parts. |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 940 NC010 PET
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Gharda Chemicals GATONE™ 5630FC Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Premix Premi-Glas® 2103-15 CRSX Polyester BMC Premi-Glas® 2103-15 CR-SX is a 15% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527 |
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c.. |
|||
Tensile Modulus | 12.0 GPa @Temperature 23.0 °C |
1740 ksi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ASTM D638 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | |
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527-2 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX8730 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8730 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-s.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527-1/-2 |
DSM Stanyl® TE250F9 (COND) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527-1/-2 |
DSM Stanyl® TW241F12 (COND) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LVX-50H black 9230 PA12-GF50 Product description: Grilamid LVX-50H black 9230 is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | cond; ISO 527-1/-2 |
DSM EcoPaXX® Q-HG10 PA410-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527 |
Eurotec® Tecopet® PT74 GR30 NL XA60 PET, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free,, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Conditioned, 40% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527-1/-2 |
Lanxess Pocan® DP T 7140 LDS 000000 PBT + PET, 44% Mineral + L227Glass Fiber
(discontinued **) PET+PBT, 44% glass fibers/mineral, injection molding, LDS, high thermal dimension stability |