| Category | Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Stanyl® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Stanyl® TW241F12 (COND) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.76 g/cc | 0.0636 lb/in³ | (DAM); ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 170 MPa | 24700 psi | ISO 527-1/-2 |
| Elongation at Break | 3.0 % | 3.0 % | ISO 527-1/-2 |
| Tensile Modulus | 12.0 GPa | 1740 ksi | ISO 527-1/-2 |
| Charpy Impact Unnotched | 10.0 J/cm² | 47.6 ft-lb/in² | ISO 179/1eU |
| 8.00 J/cm² @Temperature -30.0 °C |
38.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 2.00 J/cm² | 9.52 ft-lb/in² | ISO 179/1eU |
| 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |