Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.17 GPa | 1330 ksi | ASTM D638 |
PolyOne LubriOne™ GF-1010 40 MS 2 HS Black 37 Polyamide 6 (Nylon 6) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | |
Plastcom SLOVAMID 6 GF 30 FRA 3 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 850°C,.. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 6 GF 30 FRG 2 PA6 reinforced with glass fiber, flame retarded PA 6 for injection molding, reinforced with 30 % glass fiber, flame retarded with halogen free flame retardant. Main features: flammability in accordance with UL 94 5 at 3.2 mm. Application for the .. |
|||
Tensile Modulus | 9.17 GPa | 1330 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 886 Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 NL WH 886 resin is a glass reinforced polyphthalamide (PPA ) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | ASTM D638 |
Plenco Valite 4100 Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac.. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP DX07035 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DX07035 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame retardant, Easy Molding, Internally Lubricated, Mold R.. |
|||
Tensile Modulus | 9.20 GPa @Temperature 100 °C |
1330 ksi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Tensile Modulus | 9.16 GPa | 1330 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive. |
|||
Tensile Modulus | 9.14 GPa | 1330 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 9.15 GPa | 1330 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | ASTM-D790 |
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | dry; ISO 527-1/-2 |
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 7523-2AM BK ND3007 33% Glass Filled PA66 (Dry) Ultramid 7523-2AM BK ND3007 is an impact modified, 33% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8267G HS BK-106 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106 is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The com.. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | ISO 527-1/-2 |
DSM Stanyl® TS250F4D Nylon 46-40% Glass Reinforced (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high tempe.. |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF Information provided by EMS Grivory |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East) LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber |
|||
Tensile Modulus | 9.20 GPa | 1330 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 3235 XF 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, improved flowability |