Category | Polymer , Thermoplastic , Nylon , Nylon 6/66 |
Manufacturer | EMS-Grivory (EMS-CHEMIE) |
Trade Name | Grivory® |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183 |
Water Absorption | 5.0 % | 5.0 % | ISO 62 |
Moisture Absorption | 1.50 % | 1.50 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0010 cm/cm | 0.0010 in/in | ISO 294-4, 2577 |
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4, 2577 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 120 MPa | 17400 psi | conditioned; ISO 527-1/-2 |
170 MPa | 24700 psi | dry; ISO 527-1/-2 | |
Elongation at Break | 3.0 % | 3.0 % | dry; ISO 527-1/-2 |
7.0 % | 7.0 % | conditioned; ISO 527-1/-2 | |
Tensile Modulus | 6.50 GPa | 943 ksi | conditioned; ISO 527-1/-2 |
9.20 GPa | 1330 ksi | dry; ISO 527-1/-2 | |
Charpy Impact Unnotched | 5.00 J/cm² | 23.8 ft-lb/in² | dry; ISO 179/1eU |
8.00 J/cm² | 38.1 ft-lb/in² | conditioned; ISO 179/1eU | |
4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU | |
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | dry; ISO 179/1eA |
1.20 J/cm² | 5.71 ft-lb/in² | conditioned; ISO 179/1eA | |
0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU | |
0.400 J/cm² @Temperature 30.0 °C |
1.90 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
Maximum Service Temperature, Air | 90.0 - 120 °C | 194 - 248 °F | long term; EMS |
200 °C | 392 °F | short term; EMS | |
Deflection Temperature at 1.8 MPa (264 psi) | 240 °C | 464 °F | ISO 75-1/-2 |
Deflection Temperature at 8.0 MPa | 110 °C | 230 °F | ISO 75-1/-2 |
Flammability, UL94 | HB | HB | IEC 60695-11-10 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | dry; IEC 60093 |
1.00e+8 ohm-cm | 1.00e+8 ohm-cm | conditioned; IEC 60093 | |
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | IEC 60093 |
Dielectric Strength | 6.00 kV/mm | 152 kV/in | dry; IEC 60243-1 |
6.00 kV/mm | 152 kV/in | conditioned; IEC 60243-1 |
Descriptive Properties | Value | Comments |
---|---|---|
Automotive | Automotive electr. and electronics, lighting | |
Powertrain and Chassis | ||
Electricals & Electronics | Electrical appliances | |
Electrical equipment | ||
Form | Granules | |
Industry & Consumer goods | Mechanical Engineering | |
Power transmission | ||
Sports & Leisure | ||
Tools & Accessories | ||
Processing | Injection Molding | |
Product Attributes | Improved friction & wear properties | |
Special Characteristics | Anti-static |