Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.70 GPa | 392 ksi | |
Plastcom SLOVALEN PC 82 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
Nilit FRIANYL A63 S Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Asia Pacific) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1,2 |
Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled Filled with minerals. Flame retardant, halogen-free (V-2)Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ASTM D638 |
North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
DSM Akulon® S223-P2 Impact Modified Nylon 66 (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1, -2; 1 mm/min |
Lanxess Pocan® B 1701 000000 PBT PBT, non-reinforced, extrusion, food contactInformation provided by LANXESS. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | |
LATI Latilub 73/13-20T POM, PTFE Filled Self-lubricating product based on Polyoxymethylene (POM). PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ASTM D638 |
Solvay Specialty Polymers Veradel® 3600RP Polyethersulfone (PESU) Veradel® 3600RP hydroxyl-functionalized polyethersulfone (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersin.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX98477 PC LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | DIN 53457 |
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Conditioned Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527-1,-2 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSS PA666 Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi.. |
|||
Tensile Modulus | 2.70 GPa @Temperature 23.0 °C |
392 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® S600LF NC010 PBT Crastin® S600LF NC010 is an unreinforced, Teflon® PTFE powder lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 3022-63 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Tensile Modulus | 2.70 - 3.10 GPa | 392 - 450 ksi | |
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 901 CB POM Copolymer unreinforced, electr. conductive POMInformation provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-2 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-2 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
Mitsubishi Xantar® C CE 407 Polycarbonate/ABS Blend Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1/-2 |
DSM Arnite® T06 202 XL (T-X01151) PBT (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 2.70 GPa | 392 ksi | ASTM D638 |
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |