| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | Qualchem Zrt. |
| Trade Name | Danamid |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Qualchem Danamid FEWLX2-25 Polyamide 6, 25% Mineral Filled.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | DIN 53479 |
| Filler Content | 23 - 27 % | 23 - 27 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 48.0 MPa | 6960 psi | 50 mm/min; ISO 527-1,2 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-1,2 |
| Tensile Modulus | 2.70 GPa | 392 ksi | ISO 527-1,2 |
| Izod Impact, Notched (ISO) | 3.40 kJ/m² <br>@Temperature 23.0 °C |
1.62 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 180 |
| Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180 |
| Charpy Impact Unnotched | 1.90 J/cm² <br>@Temperature 23.0 °C |
9.04 ft-lb/in² <br>@Temperature 73.4 °F |
DIN 53453 |
| 1.90 J/cm² <br>@Temperature -30.0 °C |
9.04 ft-lb/in² <br>@Temperature -22.0 °F |
DIN 53453 | |
| Charpy Impact, Notched | 0.330 J/cm² <br>@Temperature 23.0 °C |
1.57 ft-lb/in² <br>@Temperature 73.4 °F |
DIN 53453 |
| 0.330 J/cm² <br>@Temperature -30.0 °C |
1.57 ft-lb/in² <br>@Temperature -22.0 °F |
DIN 53453 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Flammability, UL94 | V-2 <br>@Thickness 4.00 mm |
V-2 <br>@Thickness 0.157 in |
MSZ 10383 |
| Glow Wire Test | 960 °C <br>@Thickness 3.50 mm |
1760 °F <br>@Thickness 0.138 in |
IEC 685-2-1 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | DIN 53482 |
| Comparative Tracking Index | 450 V | 450 V | IEC 112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | 2.0 - 2.2 % | 2.0 - 2.2 % | DIN 53714 |