Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical Resistance Good Surface Release properties Tg of 224°C Expected Continuous Temperature of 180°C Applications: Food Contact Medical Electrical and Electronics Auto Information provided by Gharda ChemicalsSolvay Advanced Polymers completed its acquisition of this product line in May 2006.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Water Absorption 0.53 %
0.53 %
24 Hours; ASTM D570
Melt Flow 13.4 - 26.8 g/10 min
<br>@Load 2.16 kg,<br> Temperature 380 °C
13.4 - 26.8 g/10 min
<br>@Load 4.76 lb,<br> Temperature 716 °F
6`; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 2.70 GPa
392 ksi
ASTM D638
Flexural Strength 120 MPa
17400 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 51.0 µm/m-°C
<br>@Temperature 20.0 °C
28.3 µin/in-°F
<br>@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 198 °C
388 °F
ASTM D648
Glass Transition Temp, Tg 225 °C
437 °F
ASTM D3482
Flammability, UL94 V-0
<br>@Thickness 0.900 mm
V-0
<br>@Thickness 0.0354 in
UL 94
Oxygen Index 39 %
39 %
ASTM D2863
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Dielectric Constant 3.5
<br>@Frequency 1e+6 Hz
3.5
<br>@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.0 kV/mm
330 kV/in
ASTM D149
Dissipation Factor 0.010
<br>@Frequency 1e+6 Hz
0.010
<br>@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 50 sec
50 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638