Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® FR15 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE144H PC FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-000/8T Acetal-Copolymer, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy 1200-15 Polycarbonate Resin Description: LUPOY PC 1200-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
LG Chemical Lupoy 1301EP22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Tensile Modulus | 2.34 GPa @Thickness 3.18 mm |
339 ksi @Thickness 0.125 in |
ASTM D638 |
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU) Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | ASTM D638 |
Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU) Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | ASTM Data |
Styron Magnum™ 758HP ABS, High Heat, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | 2 in/min; ASTM D638 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-15 Polycarbonate EMERGEâ„¢ PC 4310-15 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Eq.. |
|||
Tensile Modulus | 2.34 GPa @Thickness 3.20 mm |
339 ksi @Thickness 0.126 in |
Injection Molded; ASTM D638 |
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can .. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Ensinger TECASON™ P MT Polyphenylsulfone (PPSU) TECASON™ P MT is a polyphenylsulfone suited primarily to applications in the medical industry. It has improved performance in terms of temperature, impact strength and chemical resistance, as well.. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Ensinger TECASON™ P Polyphenylsulfone (PPSU) TECASON™ P is a polyphenylsulfone that exhibits excellent temperature, impact and chemical resistance properties. |
|||
Tensile Modulus | 2.34 GPa | 340 ksi | ASTM D638 |
Asahi Kasei Thermylene® P-10FG-2100 10% Glass Fiber Reinforced Information provided by Asahi Thermofil |
|||
Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |