Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU)

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Solvay Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptional hydrolytic stability and toughness superior to other commercially-available, high-temperature engineering resins. They also offer high deflection temperatures and outstanding resistance to environmental stress cracking. Radel® polymers are inherently flame retardant, provide excellent thermal stability and possess good electrical properties.Features: Acid Resistant; Autoclave Sterilizable; Base Resistant; Biocompatible; E-beam Sterilizable; Ethylene Oxide Sterilizable; Flame Retardant; Good Chemical Resistance; Good Sterilizability; Good Thermal Stability; Heat Sterilizable; High ESCR (Stress Crack Resist.); High Heat Resistance; Hydrolytically Stable; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable; Ultra High ToughnessUses: Aerospace Applications; Aircraft Applications; Automotive Applications; Dental Applications; Food Service Applications; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Surgical InstrumentsAdditional Properties: Steam Sterilization - > 1000 CyclesAutomotive Specifications ASTM D6394 SP0313Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Water Absorption 0.37 %
<br>@Time 86400 sec
0.37 %
<br>@Time 24.0 hour
ISO 62
Water Absorption at Saturation 1.1 %
1.1 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm
<br>@Thickness 3.18 mm
0.0070 in/in
<br>@Thickness 0.125 in
Melt Flow 20 - 28 g/10 min
<br>@Load 5.00 kg,<br> Temperature 365 °C
20 - 28 g/10 min
<br>@Load 11.0 lb,<br> Temperature 689 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 69.6 MPa
<br>@Thickness 3.18 mm
10100 psi
<br>@Thickness 0.125 in
ASTM D638
Elongation at Break 60 - 120 %
<br>@Thickness 3.18 mm
60 - 120 %
<br>@Thickness 0.125 in
ASTM D638
Elongation at Yield 7.2 %
<br>@Thickness 3.18 mm
7.2 %
<br>@Thickness 0.125 in
ASTM D638
Tensile Modulus 2.34 GPa
<br>@Thickness 3.18 mm
339 ksi
<br>@Thickness 0.125 in
ASTM D638
Flexural Strength 91.0 MPa
<br>@Strain 5.00 %,<br> Thickness 3.18 mm
13200 psi
<br>@Strain 5.00 %,<br> Thickness 0.125 in
ASTM D790
Flexural Modulus 2.41 GPa
<br>@Thickness 3.18 mm
350 ksi
<br>@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 6.90 J/cm
<br>@Thickness 3.18 mm
12.9 ft-lb/in
<br>@Thickness 0.125 in
ASTM D256
Tensile Impact Strength 399 kJ/m²
<br>@Thickness 3.18 mm
190 ft-lb/in²
<br>@Thickness 0.125 in
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
<br>@Thickness 3.18 mm
31.1 µin/in-°F
<br>@Thickness 0.125 in
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
<br>@Thickness 3.20 mm
405 °F
<br>@Thickness 0.126 in
Unannealed; ASTM D648
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Flammability, UL94 V-0
<br>@Thickness 0.762 mm
V-0
<br>@Thickness 0.0300 in
Optical Properties Metric English Comments
Refractive Index 1.672
1.672
ASTM D542
Electrical Properties Metric English Comments
Volume Resistivity 9.00e+15 ohm-cm
9.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.44
<br>@Frequency 6.00e+7 Hz
3.44
<br>@Frequency 6.00e+7 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
<br>@Thickness 3.18 mm
381 kV/in
<br>@Thickness 0.125 in
ASTM D149
>= 200 kV/mm
<br>@Thickness 0.0254 mm
>= 5080 kV/in
<br>@Thickness 0.00100 in
ASTM D149
Processing Properties Metric English Comments
Melt Temperature 360 - 391 °C
680 - 736 °F
Mold Temperature 138 - 163 °C
280 - 325 °F
Drying Temperature 149 °C
300 °F
171 °C
<br>@Time 14400 sec
340 °F
<br>@Time 4.00 hour
Descriptive Properties Value Comments
Agency Ratings ISO 10993
Availability Asia Pacific
Europe
Latin America
North America
Color Clear Amber; Colors
Form Pellets
Processing Technique Extrusion; Injection Molding
Sheet Extrusion; Thermoforming
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.2:1.0