| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® ML6031 PC Copolymer (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D 792 |
| Density | 1.20 g/cc | 0.0434 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.15 % | 0.15 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.35 % <br>@Temperature 23.0 °C |
0.35 % <br>@Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 5.0 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
5.0 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| 6.0 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
6.0 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ASTM D 1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 76.0 MPa | 11000 psi | Type I, 50 mm/min; ASTM D 638 |
| 76.0 MPa | 11000 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 67.0 MPa | 9720 psi | Type I, 50 mm/min; ASTM D 638 |
| 67.0 MPa | 9720 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | >= 100 % | >= 100 % | Type I, 50 mm/min; ASTM D 638 |
| >= 100 % | >= 100 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 6.3 % | 6.3 % | Type I, 50 mm/min; ASTM D 638 |
| 6.3 % | 6.3 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.34 GPa | 339 ksi | 5 mm/min; ASTM D 638 |
| 2.34 GPa | 339 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 96.0 MPa | 13900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
| 96.0 MPa | 13900 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
| 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 1.40 J/cm <br>@Temperature -30.0 °C |
2.62 ft-lb/in <br>@Temperature -22.0 °F |
ASTM D 256 |
| 8.20 J/cm <br>@Temperature 23.0 °C |
15.4 ft-lb/in <br>@Temperature 73.4 °F |
ASTM D 256 | |
| Impact Test | 85.0 J <br>@Temperature 23.0 °C |
62.7 ft-lb <br>@Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 70.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 70.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 121 °C | 250 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 134 °C <br>@Thickness 3.20 mm |
273 °F <br>@Thickness 0.126 in |
unannealed; ASTM D 648 | |
| Vicat Softening Point | 135 °C | 275 °F | Rate B/50; ASTM D 1525 |
| 137 °C | 279 °F | Rate B/50; ISO 306 | |
| 139 °C | 282 °F | Rate B/120; ISO 306 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Haze | 0.50 % <br>@Thickness 2.54 mm |
0.50 % <br>@Thickness 0.100 in |
ASTM D 1003 |
| Transmission, Visible | 89 % <br>@Thickness 2.54 mm |
89 % <br>@Thickness 0.100 in |
ASTM D 1003 |