Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON TR1000 PMMA+CNT Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG .. |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GP2102 PC+GF10% Description: Injection Molding, PC+GF10%, General Purpose, Good Toughness, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GP5008BFH PC/ABS, Flame Retardance Description: Injection Molding, PC/ABS, Flame Retardance, High Flow, Heat Resistant, High Impact Application: E&E (Housing)Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY HI5002A PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY SC1004AU PC, High Impact Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat.. |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa @Thickness 3.20 mm |
7970 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical XG569C MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 54.9 MPa | 7970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 54.9 MPa | 7970 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 54.9 MPa | 7970 psi | ASTM D638 |
Samyang Tribit® 1500 Polybutylene Terephthalate Characteristics:Medium viscosityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samy.. |
|||
Tensile Strength, Yield | 54.9 MPa | 7970 psi | ASTM D638 |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Tensile Strength, Yield | 54.9 MPa | 7970 psi | ASTM D638 |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Tensile Strength, Yield | 54.9 MPa | 7970 psi | ASTM D638 |
Cheng Yu Plastic B610 PC/PBT |
|||
Tensile Strength, Yield | 54.9 MPa | 7970 psi | ASTM D638 |
Cheng Yu Plastic E500 PC/PET |