| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.20 g/cc | 1.20 g/cc | ASTM D792 |
| Linear Mold Shrinkage | 0.0060 - 0.0080 cm/cm | 0.0060 - 0.0080 in/in | ASTM D955 |
| Melt Index of Compound | 16 g/10 min | 16 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 90 | 90 | ASTM D785 |
| Tensile Strength, Yield | 54.9 MPa | 7970 psi | ASTM D638 |
| Flexural Yield Strength | 96.1 MPa | 13900 psi | ASTM D790 |
| Izod Impact, Notched | 85.0 J/cm | 159 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 110 °C | 230 °F | ASTM D648 |
| Flammability, UL94 | HB | HB |