Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min; ISO 527 |
Polimeri Europa Edistir RK 5512G Polystyrene UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal properties. It exhibits a good stability to the processing conditions and to the light
exposure.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
SABIC M40053S High Density Polyethylene for Injection Molding Product Description: M40053S is a UV stabilized high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to pro.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50mm/min; ASTM D638 |
Reliance Industries Repol C080MA Polypropylene REPOL Polypropylene C080MA is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Global GA-3245 High Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- shopping bags, packing bagsInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 23.0 MPa @Thickness 3.20 mm |
3340 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-4630 GFR Flame Retarded Polypropylene Block-Copolymer INNOPOL® CS 2-4630 GFR is a flame retarded polypropylene block-copolymer compound. This grade is available in nature and custom colored form.INNOPOL® CS 2-4630 GFR is recommended for producing.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638-02 |
Ipiranga Petrochem GM 9245 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Micropol Isoplas P381 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Tensile Strength, Yield | >= 23.0 MPa | >= 3340 psi | 50 mm/min; ISO 527 |
MTM Plastics Purpolen® PE Polyethylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
LyondellBasell Astryn SB572C Polypropylene Copolymer Key Features: fractional melt flow, medium modulus, extrusion grade polypropylene copolymer, good melt strength, good processabilityApplications: solar panelsDescription: Astryn SB572C fractional me.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527-1, -2 |
LyondellBasell Hifaxâ„¢ RTA3263EUV/1 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ RTA3263EUV/1 fractional melt flow, 1,700 MPa flexural modulus, UV-stabilized, mineral-filled, extrusion grade thermoplastic elastomeric olefin (TEO) resin has an excellent b.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP TX97446 PU LNP* LUBRICOMP* TX97446 is a compound based on Polyurethane containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | Crosshead speed 100 mm/min; ISO 527 |
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | Crosshead speed 100 mm/min; ISO 527 |
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527-2 |
Borealis Borpact™ SG910MO Polypropylene for Injection Molding Borpact™ SG910MO is a high impact and transparent polypropylene. This grade provides high gloss, high transparency and excellent impact properties. Applications: containers and products with medium.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
Unipetrol PP MONSTEN® MA 611 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
Unipetrol PP MONSTEN® MA 612 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527-2 |
Total PPC 9712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Entec Hypro™ PP-CP35/2 Impact Copolymer, 35 Melt Flow This product is intended for general purpose injection molding applications including consumer products, housewares and packaging.Information provided by Entec |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Braskem GM5340PR High Density Polyethylene Triple-layer coating for metallic pipes; Umbilical pipes for offshore oil field platforms; Jacketing for wires and for optic fiber metallic cables; Self-propelled irrigation pipes; Localized irrigat.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM-D638 |
Braskem GM7040G HDPE High Density Extrusion Polyethylene GM7040G is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for a gas pressurized line. It is produced with bimodal technology and has high molar mass.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436T40L1 Talc Reinforced |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | |
BASF Novolen® 2500 H Polypropylene Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | |
BASF Procom® D 1158 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 23.0 MPa @Temperature 121 °C |
3340 psi @Temperature 250 °F |
ISO 527 |
BASF Ultramid® 8200 HS PA 6 (Dry) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
Aclo Accutech Polypropylene Copolymer CP0436T20L1 Talc Reinforced |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min; ASTM D638 |
Carmel Olefins CAPILENE® SR 50 Polypropylene Impact Copolymer Description: CAPILENE® SR 50 is a medium melt flow rate impact copolymer for injection molding applications. This grade offers good balance of stiffness, impact strength and processability.Applic.. |
|||
Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
NOVA Chemicals Sclair® 97B HDPE Blow Molding Resin
(discontinued **) Features: Good impact strength, easy processability, high ESCR.Applications: Small part blow molding, high ESCR HIC applications.Data provided by the manufacturer. |