| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
SABIC M40053S High Density Polyethylene for Injection Molding
Product Description: M40053S is a UV stabilized high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to pro..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
North Wood Plastics PS with 20% Wood Fiber
Data provided by North Wood Plastics, Inc.
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50mm/min; ASTM D638 |
|
Reliance Industries Repol C080MT Polypropylene
REPOL Polypropylene C080MT is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min |
|
Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)
(discontinued **)
Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-23 UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal pr..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
Chevron Phillips HiD® 9348 HDPE Natural Pipe Resin
(discontinued **)
Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification: 335440A; ASTM D 4976 Classification: PE 235, A 56606Applications:Base Resin for use in Oil Patch and Industrial Pipe Appl..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min |
|
Eastman Tenite 264-16 CAB Cellulose Acetate Butyrate
(discontinued **)
16% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
|
Fiberfil® M-2450 BK9083 Polypropylene Copolymer, 20% Talc
Information provided by FIBERFIL Engineered Plastics
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
|
Manifattura Cattaneo PE HD Polyethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
|
|||
| Tensile Strength, Yield |
23.0
MPa @Thickness 3.20 mm |
3340
psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
|
LG Chemical HIPS 460AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
Global GG-3245 High Density Polyethylene, Blow Molding Grade
Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- auto parts, bottles, housewares, drums, containers, bottlesInformation provided by Global Poly..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638-02 |
|
Ipiranga Petrochem GM 5010 T2 HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638-02 |
|
Ipiranga Petrochem GM 9245 F HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | 50 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP THERMOCOMP C1000XXP PS (Europe-Africa-Middle East)
LNP* THERMOCOMP* C1000XXP is a compound based on Polystyrene resin. Added features include: High Impact.
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | |
|
Silon Tabond 3012 Adhesive Resin
TABOND 3012 is an LLDPE based adhesive resin.Characteristics: • Highest adhesion to aluminium, copper, brass and steel • Adhesion durability at elevated temperatures and pressure cycling p..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
|
Unipetrol PE HD LITEN® FB 75 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
Total PPC 5571 Polypropylene, Impact Copolymer Injection Molding
TOTAL Petrochemicals Polypropylene 5571 is a high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 5571 is characterized by significantly improved impact resistance, while m..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527-2 |
|
Total PPC 9712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527-2 |
|
Total PPC 11750 Polypropylene, Heterophasic Copolymer, Injection Molding
Polypropylene PPC 11750 is a nucleated and controlled-rheology heterophasic copolymer with very high Melt Flow index of 50 g/10 min.Polypropylene PPC 11750 is characterized by good impact resistance..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
Videolar 825 E High Impact Polystyrene (HIPS)
Grade designed specially for extrusion and thermoformingCharacteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusionFeatures: St..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527-2/50 |
|
ExxonMobil PP7054L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with medium flow. It is suitable for molding applications like consumer products, closures, containers, toys and rigid packaging applications..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | Typical; ISO 527-1/2 |
|
Axion Polymers Axpoly® PS02 1010 Medium Impact Polystyrene
PS02 Series polystyrenes offers the designer and processor a high performance polymer with well-defined properties in a range of options to suit many applications.The Axpoly® PS02 range of resin co..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | Typical; ISO 527-1/2 |
|
Axion Polymers Axpoly® PS13 Impact Modified Polystyrene
100% post-consumer recycled polymer (recovered from coat hangers)93% less CO2 impact compared with virgin*Successfully replaces virgin grade resinISO9000 quality certifiedAvailable in black/greyCost..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | Yield, 50/50 mm/min; ISO 527-1 |
|
Addcomp PRIEX® 12031 Maleic Anhydride Grafted HDPE
Fields of application: Functionalised polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to r..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO R527 |
|
Arkema Group Orgalloy® LT 5050 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
Braskem CP 141 Injection Molding Polypropylene
Description: CP 141 is a high melt flow rate heterophasic copolymer specially designed to achieve high productivity on thin-walled parts with very easy mould filling and high speed injection mouldin..
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
Aclo Accutech Polypropylene Copolymer CP0436T10L1 Talc Reinforced |
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
|
NOVA Chemicals Sclair® 97B HDPE Blow Molding Resin
(discontinued **)
Features: Good impact strength, easy processability, high ESCR.Applications: Small part blow molding, high ESCR HIC applications.Data provided by the manufacturer.
|
|||
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ISO 527 |
|
Unipetrol PE HD LITEN® MB/ML 57 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
|
|||