LyondellBasell Astryn SB572C Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LyondellBasell Astryn SB572C Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: fractional melt flow, medium modulus, extrusion grade polypropylene copolymer, good melt strength, good processabilityApplications: solar panelsDescription: Astryn SB572C fractional melt flow, precolored, extrusion grade polypropylene copolymer has balanced strength and processability.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792B
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Tool, Montell
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.0 MPa
4930 psi
ASTM D638
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 5.30 J/cm
9.93 ft-lb/in
ASTM D256A
Gardner Impact 36.0 J
26.6 ft-lb
ASTM D3029