Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DFP22 PC LNP* DFP22 is a Polycarbonate base resin containing glass fiber and PTFE/Silicone Lubricants. Characteristic of this grade is: Internally Lubricated.This data was supplied by SABIC-IP for the Amer.. |
|||
Tensile Strength, Yield | 73.1 MPa | 10600 psi | ASTM D638 |
Omni Plastics OmniLon™ 6 PA6 WF10 Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 73.1 MPa | 10600 psi | ASTM D638 |
Omni Plastics OmniLon™ 6 PA6 WF30 Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK LNP* LUBRICOMP* LL004E is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP UAL22S PPA LNP* LUBRICOMP* UAL22S is a compound based on Polyphthalamide resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp GX061104 PSU (Europe-Africa-Middle East) LNP* COLORCOMP* GX061104 is a compound based on Polysulfone resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East) LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 73.1 MPa | 10600 psi | ASTM D638 |
Washington Penn Polypropylene Copolymer 30% Glass Reinforced Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 50 mm/min; ISO 527 |
Eurostar Starglas GX061104 PSU Starglas GX061104 is a PSU resin (also known as Starglas PSU A ¾)Information provided by Eurostar. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, Conditioned Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 300 MW4 POM Mineral filled injection molding grade based on Tarnoform 300 reinforced with 20% wollastonite; such a compound has high stiffness, dimensional stability and hardness combined with low shrinkage.Inf.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® SC631 NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium-high Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC631 is a medium-high viscosity acetal homopolymer developed for parts requiring high precision moldi.. |
|||
Tensile Strength, Yield | 73.0 MPa @Temperature 23.0 °C |
10600 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
Tensile Strength, Yield | 73.0 MPa @Temperature 23.0 °C |
10600 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp TX88477 PU LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Tensile Strength, Yield | 73.0 MPa @Temperature 23.0 °C |
10600 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® SC631 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® SC631 is a medium-high viscosity acetal homopolymer, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Tensile Strength, Yield | 73.0 MPa | 10600 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
Tensile Strength, Yield | 73.3 - 160 MPa | 10600 - 23200 psi | Average value: 128 MPa Grade Count:4 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |