Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ASTM D638 |
Plaskolite Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | chs 2 in/min; ASTM D638 |
Network Polymers SAN 278 Medium Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ASTM D638 |
Plaskolite West Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line. |
|||
Tensile Strength, Yield | 71.5 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal Homopolymer
(Unverified Data**) Delrin® 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro.. |
|||
Tensile Strength, Yield | 72.0 MPa @Thickness 6.35 mm |
10400 psi @Thickness 0.250 in |
ASTM D638 |
SABIC Innovative Plastics Lexan® FL933 PC Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized. |
|||
Tensile Strength, Yield | 71.6 MPa @Thickness 3.20 mm |
10400 psi @Thickness 0.126 in |
ASTM D638 |
LG Chemical LUMILOY GN1306F Injection Molding FR Heat Resistant mPPO Uses include electric/electronic parts. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 2 in/min; ASTM Test |
Styrolution Luran® 358 N SAN Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Asia Pacific) |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | ASTM D638 |
Sumitomo Chemical Sumipex® MH Acrylic Resin, Heat Resistant Product CharacteristicsExtrusion GradeHeat ResistantInformation provided by Calsak Corporation |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-2 |
Tisan TISAPET® 20% Glass Reinforced Polyethylene Terephthalate Properties:Excellent mechanical propertiesHigh thermal-chemical friction resistanceGood electrical propertiesGood rate of melt flow index relative to the quantity of glass fiberBalanced electrical a.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-2 |
Tisan TISLAMID® 6 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® 1800 Polycarbonate Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® DP1-9354/1 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/3,2mm (UL 94)V-2/1,5mm (UL 94),softening temperature (VST/B 120)=185 °Calso available in transparent colorsPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers with very low VOC emissi.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® II150E BK602 Acetal (POM) Nucleated High Viscosity Acetal Homopolymer Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 71.7 MPa | 10400 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers NPP 60-8419G Clear Amorphous Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact ApplicationsDelrin FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. I.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 MCS I8 Polyamide 6 - Impact Modified Increased impact resistance grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main propert.. |
|||
Tensile Strength, Yield | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral. |
|||
Tensile Strength, Yield | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |