Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ASTM D638 |
Plaskolite Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Europe-Africa-Middle East) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer High viscosity Proprietary Polycarbonate Ester, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ASTM D638 |
Plaskolite Optix® SG Sign Grade Acrylic Sheet Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Tensile Strength, Yield | 72.0 MPa @Thickness 6.35 mm |
10400 psi @Thickness 0.250 in |
ASTM D638 |
SABIC Innovative Plastics Lexan® FL930 PC Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Tensile Strength, Yield | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 2 in/min; ASTM Test |
Styrolution Luran® 358 N SAN Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527 |
Styrolution Luran® HD 20 SAN Luran HD 20 is an easy-flow grade of SAN especially designed for the medical market. It is suitable for moldings with very thin walls and / or adverse flow length to wall ratio. It features very goo.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific) PPO/PS unfilled high heat |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Tensile Strength, Yield | 72.0 MPa @Thickness 6.35 mm |
10400 psi @Thickness 0.250 in |
ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM3020 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_FM3020 compound is GR/MR 30%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Europe-Africa-Middle East) |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
Covestro Apec® DP1-9354/1 Polycarbonate, Flame Retardant Grade Developmental productflame retardant: V-0/3,2mm (UL 94)V-2/1,5mm (UL 94),softening temperature (VST/B 120)=185 °Calso available in transparent colorsPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers with very low VOC emissi.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal (POM) Nucleated Low Viscosity Acetal Homopolymer with Low Screw DepositInformation provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® SZ800 Modified Polyphenylene Ether High-Heat ResistantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | ISO value at 50 mm/min. |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral. |
|||
Tensile Strength, Yield | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |
|||
Tensile Strength, Yield | 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® SD9705 PC Copolymer (Europe-Africa-Middle East) High visocisty PC Copolymer, low smoke, flame retardant resinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |