Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Tensile Strength, Yield | 39.0 - 50.0 MPa | 5660 - 7250 psi | Average value: 44.8 MPa Grade Count:4 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tensile Strength, Yield | 39.0 - 52.0 MPa | 5660 - 7540 psi | Average value: 46.5 MPa Grade Count:6 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638-02 |
Ipiranga Petrochem PH 0141 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copolymer LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant... |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 337 PBT Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp 5X06476 FP-V (PVDF) LNP* FP-VM-3830 is a compound based on Polyvinylidine Fluoride (PVDF) containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527-1,-2 |
Styrolution Novodur® P2M-AT ABS Pellets Novodur® P2M-AT has high impact strength, high gloss, and contains antistatic additive. It is used for the production of molded plastic articles. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527-2/50 |
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 100mm/min; ISO 527-2 |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL 844 PPE+PS (Asia Pacific) Medium heat PPO/HIPS alloy used in the automotive industry. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
Unipetrol PP MONSTEN® MT 230 Polypropylene Homopolymer Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 39.0 MPa @Strain 300 % |
5660 psi @Strain 300 % |
ISO 527-1/-2 |
Covestro Desmopan® DP 8798A S043 Polyurethane PreprocessingMax. Water content |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Entec Hypro™ PP-HP20NS Homopolymer, 20 Melt Flow, Nucleated, Anti-stat This product is intended for general purpose injection molding applications such as cutlery, caps and closures, and thin-wall containers.Information provided by Entec |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-764 ABS - Flame Retardant F.R. Weather Resistant |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Braskem H 502 HC Injection Molding Polypropylene Description: H 502HC is a low melt flow rate homopolymer, designed for very high stiffness/toughness applications with good processability. This product exhibits excellent chemical resitance and bar.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Ashley Polymers Ashlene® R3144 PC/PBT A thermoplastic alloy offering a high level of chemical resistance combined with high impact and excellent mechanical properties. Black.Data provided by the manufacturer |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min |
Arkema Group Rilsan® AMN D Nylon 12, Rigid, Injection Grade (Conditioned) Designation ISO 1874-PA12,MR,14-010Rigid grade for injection molding. Available colors: black, natural, orange, red and white. Possibilities of heat and light stabilizing agents. Mold-release agent... |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min |
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® 100Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Ineos H05Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Closures, DispensersComplies with FDA specification, Title 21, CFR 177.1520.Typical property data.. |