| Category | Polymer , Thermoplastic , Polyolefin , Polyphenylene Ether/PPO |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
| Melt Flow | 20.2 g/10 min @Load 5.00 kg, Temperature 280 °C |
20.2 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
| Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 280 °C |
20 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 65 | 65 | 30S reading; ASTM D2240 |
| Tensile Strength at Break | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
| 37.0 MPa | 5370 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 37.0 MPa | 5370 psi | Type I, 50 mm/min; ASTM D638 |
| 39.0 MPa | 5660 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 38 % | 38 % | 50 mm/min; ISO 527 |
| 45 % | 45 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 17 % | 17 % | 50 mm/min; ISO 527 |
| 37 % | 37 % | Type I, 50 mm/min; ASTM D638 | |
| Tensile Modulus | 1.45 GPa | 210 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 41.0 MPa | 5950 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 44.0 MPa | 6380 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 1.15 GPa | 167 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 1.26 GPa | 183 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
| Izod Impact, Notched (ISO) | 41.0 kJ/m² | 19.5 ft-lb/in² | 80*10*4; ISO 180/1A |
| 9.00 kJ/m² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 4.30 J/cm² | 20.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 33.0 J @Temperature 23.0 °C |
24.3 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| 42.0 J @Temperature -30.0 °C |
31.0 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 82.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 131 µm/m-°C @Temperature -40.0 - 40.0 °C |
72.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| Deflection Temperature at 0.46 MPa (66 psi) | 115 °C @Thickness 3.20 mm |
239 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 93.0 °C | 199 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 84.0 °C @Thickness 3.20 mm |
183 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 71.0 °C | 160 °F | Rate B/50; ASTM D1525 |
| 71.0 °C | 160 °F | Rate B/50; ISO 306 | |
| 76.0 °C | 169 °F | Rate B/120; ISO 306 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 2.5 @Frequency 1.00e+6 Hz |
2.5 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dissipation Factor | 0.0020 @Frequency 1.00e+6 Hz |
0.0020 @Frequency 1.00e+6 Hz |
IEC 60250 |