Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin Features: Excellent balance of stiffness and toughness, low odor.Applications: Margarine and spreads, thin walled containers, frozen food containers.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM Data |
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene
(discontinued **) STYRON 8100 MFD high impact polystyrene is designed for microfloppy diskettes (MFD) applications. It offers easy processing, coloring, abrasion resistance, impact strength, and high heat resistance... |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50 mm/min test speed; ASTM D 638 |
NOVA Chemicals Sclair® IG464-C Injection Molded HDPE Resin IG464-C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG464.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Global PP-2300-LC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638-02 |
Ipiranga Petrochem GM 8250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Tensile Strength, Yield | 27.0 MPa @Strain 0.200 %, Temperature 1095 °C |
3920 psi @Strain 0.200 %, Temperature 2003 °F |
|
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | BP 13B/1 |
SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50 mm/min; ISO 527-1/-2 |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50mm/min; ISO 527-2 |
Borealis BD950MO Polypropylene Copolymer BD950MO is a heterophasic copolymer. This grade is intended for compression and injection molding. The main features of this grade are good stiffness and impact resistance, very good process ability.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50mm/min; ISO 527-2 |
Borealis BorPURE™ RG466MO Polypropylene, Transparent Random Copolymer BorPure™ RG466MO is a specially modified high MFR transparent polypropylene random copolymer based on proprietary Borealis Nucleation Technology (BNT), with an excellent organoleptic performance. N.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200X is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527-2 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527-2 |
Total PPC 5752 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 5752 is a nucleated controlled-rheology heterophasic copolymer. PPC 5752 is characterized by a high impact resistance and excellent antistatic properties. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ISO 527-2 |
Total PPC 7612 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 7612 is a nucleated and controlled-rheology heterophasic copolymer. PPC 7612 is characterized by a good balance between rigidity and impact resistance and has excellent antistatic.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50mm/min; ISO 527-2 |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1285H Glass Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP 1285H is a 20% glass reinforced copolymer polypropylene compound. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50 mm/min; ISO 527 |
Chi Mei Polyrex® PH-60 Polystyrene - High Impact Medium impact |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50 mm/min; ISO 527 |
Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Global NM-3255 High Density Polyethylene, Yarn/Tape Grade
(discontinued **) Description-opacity, medium high stiffness, good impact strength, good chemical resistanceApplications- ropes, fishing nets, wire & cable insulators, auto parts, pipesInformation provided by Global .. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | |
Addcomp PRIEX® Ionomer 45101 PP random copolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
Ineos Nova 5620 High Impact Polystyrene
(discontinued **) High heat resistance, Good balance of toughness and rigidityApplications: Food service itemProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.I.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFLAM™ RPP 1021 General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1021 is a general purpose copolymer polypropylene flame retardant material with a UL V-2 flammability rating and 105°C temperature index at 0.030 in.Information provided b.. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 50 mm/min |
Arkema Group Orgalloy® LT 6040 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |
|||
Tensile Strength, Yield | 27.0 MPa | 3920 psi | 2 in/min, Type IV bar; ASTM D-638 |
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE High density polyethylene. This high molecular weight, hexene copolymer with synthetic antistatic agent is tailored for lightweight blow molded containers that: Require excellent stiffnessRequire .. |