Addcomp PRIEX® Ionomer 45101 PP random copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Addcomp
Trade Name PRIEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp PRIEX® Ionomer 45101 PP random copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce thickness in multi-layer films or pipesIncrease elongation resistance in polyolefin fibersAct as a nucleating agent in polyolefinsEnhance creep resistance in pipesReinforce strain hardening in polyolefinsImprove compatibility between different polymersIncrease oxidation resistance in polyolefinsInformation provided by Addcomp Polymer Additive Solutions
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
Elongation at Break >= 600 %
>= 600 %
Tensile Modulus 0.800 - 0.900 GPa
116 - 131 ksi
Thermal Properties Metric English Comments
Melting Point 135 - 137 °C
275 - 279 °F
Crystallization Temperature 93.0 - 97.0 °C
199 - 207 °F
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
Descriptive Properties Value Comments
Oxygen induction time >80 min